首页> 外国专利> Blow-moulded or injection-moulded polypropylene@ mouldings with balance stiffness and heat distortion temperature

Blow-moulded or injection-moulded polypropylene@ mouldings with balance stiffness and heat distortion temperature

机译:吹塑或注塑聚丙烯@模塑件,具有平衡的刚度和热变形温度

摘要

Blow-moulded or injection-moulded polyolefin mouldings with improved heat distortion temperature and stiffness comprise: (a) 60-99.9, preferably 75-98 wt.% unmodified polypropylene polymer (I) and (b) 40-0.1, preferably 25-2 wt.% modified propylene polymer (B). (I) consists of (a1) usual propylene polymers, preferably homopolymers produced using Ziegler-Natta or metallocene catalyst, especially with a weight/number average molecular weight ratio Mw/Mn of 2-4.5, and/or random, block and/or random block copolymers of 80.0-99.9 wt.% propylene with ethylene and/or 4-18 carbon (C) alpha -olefins with a melt index (MI; g/10 min at 230 deg C/2.16 kg) = 0.1-300, preferably 1-100,; (a2) a polyolefin mixture, with Mw/Mn = 2-6 and MI = 1-40, of (a2.1) 60-98 wt.% crystalline copolymer of 85-99.5 wt.% propylene and 15-0.5 wt.% ethylene and/or alpha -olefin of the formula CH2=CHR (R = linear or branched 2-8 alkyl); (a2.2) 2-40 wt.% elastic copolymer of 20-70 wt.% ethylene and 80-30 wt.% propylene and/or CH2=CHR; (a3) amorphous (co)polypropylene containing 0-20 wt.% CH2=CHR, with 10 wt.% crystalline fraction with a melt enthalpy 40 J/g and MI = 0.1-100; (a4) non-isotactic homopolypropylene with a melting point of 145-165 deg C, heat of crystallisation of 4-10 cal/g and 35-55 wt.% soluble fraction in diethyl ether. (I) contains 0.01-2.5 wt.% stabiliser, 0.01-5 wt.% processing aid and optionally 0.1-1 wt.% antistatic, 0.2-3 wt.% pigment, 0.05-1 wt.% nucleating agent, 2-20 wt.% flame retardant as ancillaries and/or 3-40 wt.% (in)organic filler(s) and/or reinforcement(s) with respect to (I). The novel features are that (i) (II) is a modified homo- and/or co-polymer with MI = 0.05-40, preferably 0.25-15 and the ratio of the intrinsic viscosity of (II) to that of the unmodified polymer of the same Mw on which it is based is 0.20-0.95; and (ii) (II) is produced by (b1) modifying homopolypropylene and/or copolymers of propylene and ethylene and/or 4-18 C alpha -olefins with polyfunctional ethylenically unsaturated monomers and/or with ionising radiation or thermal free radical initiators; (b2) reacting functionalised polypropylene, preferably containing acid and/or acid anhydride groups, with polyfunctional compounds of opposite reactivity, preferably 2-16 C diamines ad/or 2-16 C diols; and/or (b3) hydrolytic condensation of polypropylene containing hydrolysable silane groups. Also claimed is a method of making the mouldings.
机译:具有改善的热变形温度和刚度的吹塑或注塑聚烯烃模制品包括:(a)60-99.9,优选75-98 wt。%的未改性聚丙烯聚合物(I)和(b)40-0.1,优选25-2重量%的改性丙烯聚合物(B)。 (I)由(a1)常用的丙烯聚合物组成,优选使用齐格勒-纳塔或茂金属催化剂生产的均聚物,特别是重均分子量数Mw / Mn为2-4.5,和/或无规,嵌段和/或80.0-99.9 wt%丙烯与乙烯和/或4-18碳(C)α-烯烃的无规嵌段共聚物,其熔体指数(MI;在230摄氏度/2.16千克时g / 10分钟)= 0.1-300,最好是1-100; (a2)Mw / Mn = 2-6和MI = 1-40的聚烯烃混合物,其中(a2.1)60-98 wt%的85-99.5 wt%的丙烯和15-0.5 wt%的丙烯的结晶共聚物。式CH 2 = CHR(R =直链或支链的2-8烷基)的%乙烯和/或α-烯烃; (a2.2)2-40重量%的20-70重量%的乙烯和80-30重量%的丙烯和/或CH 2 = CHR的弹性共聚物; (a3)非晶态(共)聚丙烯,其包含0-20重量%的CH 2 = CHR,具有10重量%的结晶级分,且熔融焓为40J / g,MI = 0.1-100; (a4)熔点为145-165℃,结晶热为4-10cal / g和35-55wt。%可溶于二乙醚的非等规均聚丙烯。 (I)包含0.01-2.5 wt。%的稳定剂,0.01-5 wt。%的加工助剂和可选的0.1-1 wt。%的抗静电剂,0.2-3 wt。%的颜料,0.05-1 wt。%的成核剂,2-20相对于(I),助剂的重量百分比为阻燃剂和/或在有机填料和/或增强材料中的含量为3-40重量%。新颖的特征是(i)(II)是MI = 0.05-40,优选0.25-15的改性均聚物和/或共聚物,并且(II)的特性粘度与未改性的聚合物的特性粘度之比它所基于的同一Mw的0.20-0.95; (ii)(II)是通过(b1)用多官能的烯键式不饱和单体和/或电离辐射或热自由基引发剂改性均聚丙烯和/或丙烯与乙烯和/或4-18 Cα-烯烃的共聚物制得的; (b2)使优选含有酸和/或酸酐基团的官能化聚丙烯与具有相反反应性的多官能化合物,优选2-16 C的二胺和/或2-16 C的二醇反应;和/或(b3)含有可水解硅烷基团的聚丙烯的水解缩合。还要求保护一种制造模制品的方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号