PROBLEM TO BE SOLVED: To provide a method for efficiently producing hydrogenated fullerene as a material for hydrogen storage and to provide a method for recovering hydrogen from the hydrogenated fullerene. SOLUTION: A transformation method comprises transforming C60 fullerene into hydrogenated fullerene and vice versa both in the presence of a Ni/Al2O3 catalyst where active alumina is impregnated with nickel to support it. This method for producing hydrogenated fullerene comprises utilizing a transformation reaction in the presence of a Ni/Al2O3 catalyst where active alumina is impregnated with nickel to support it in order to transform C60 fullerene into hydrogenated fullerene C60H36 under a mildly hydrogenating condition at high efficiency and selectivity.
机译:解决的问题:提供一种有效地生产氢化富勒烯作为储氢材料的方法,并提供一种从氢化富勒烯中回收氢的方法。解决方案:一种转化方法包括在Ni / Al2O3催化剂存在下将C60富勒烯转化为氢化富勒烯,反之亦然,其中活性氧化铝用镍浸渍以负载它。该生产氢化富勒烯的方法包括在Ni / Al2O3催化剂存在下利用转化反应,其中活性氧化铝用镍浸渍以支撑它,以便在温和的氢化条件下以高效率和选择性将C60富勒烯转化为氢化富勒烯C60H36。 。

著录项

  • 公开/公告号JP3066495B1

    专利类型

  • 公开/公告日2000-07-17

    原文格式PDF

  • 申请/专利权人 工業技術院長;

    申请/专利号JP19990082789

  • 发明设计人 尾崎 利彦;多井 豊;

    申请日1999-03-26

  • 分类号C01B31/02;C01B3/00;C07C1/00;C07C13/32;

  • 国家 JP

  • 入库时间 2022-08-22 02:06:02

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号