首页> 外国专利> Materials espumados polyurethane semi-rigid base poliisocionatos modified with biuret.Composite structural components using these materials espumados semi rigid polyurethane and a process for its production.

Materials espumados polyurethane semi-rigid base poliisocionatos modified with biuret.Composite structural components using these materials espumados semi rigid polyurethane and a process for its production.

机译:使用缩二脲改性的材料espumados聚氨酯半刚性基础poliisocionatos。使用这些材料的espumados半刚性聚氨酯复合结构部件及其生产方法。

摘要

Invention patent: b "materials espumados polyurethane semi ru00ecgidos based poliisociantos modified with biuret.Composite structural components using these materials espumados semi ru00ecgidos polyurethane and a process for the production of " d .Polyurethane materials are described espumados, semi rigid, which have a density of 60.1 to 200 kg / m3.These materials espumados are available by reaction of (a) a poliisocianato component, which has an NCO content of from 30 to 47%.And which comprises a disocianato toluene which has a structure of biuret, and which has a value of NCO within the range of 33 to 47% by weight,(b) a polyester polyol component with an average molecular weight of 1000 to 12.000 and a feature 242 2, (c) from 0.5 to 8% by weight of water based on the total weight of components (b), (c), (d), (E) and (f), (d) optionally.An additional component of polyol with an average molecular weight of 62 to less than 1.000 and a feature 242 2, (E) optionally with substances admixtures, additives and flame retardants, additional known in technique, and optionally (F0, blowing agents,While it remains an isocyanate index of 30 to 180 with respect to the ratio of isocyanate groups in the component (a) to the sum of the reactive with isocyanate groups present in the components (b)And (f). A process for the production of such materials espumados and its use in composite structural components are also described.
机译:发明专利:材料用双缩脲改性的基于espumados的聚氨酯半聚醚基多聚体。使用这些材料的复合结构组分和生产聚氨酯的方法。描述了聚氨酯材料半硬质espumados,密度为60.1至200 kg / m3。这些材料espumados可通过(a)NCO含量为30%至47%的poliisocianato组分反应获得。甲苯,具有缩二脲结构,NCO值在33%至47%的范围内。(b)平均分子量为1000至12.000且特征<242> 2的聚酯多元醇组分, (c)基于组分(b),(c),(d),(E)和(f),(d)的总重量的0.5至8%的水。平均分子量为62至小于1.000,特征<242> 2,(E)可选在技​​术上是已知的其他物质的混合物,添加剂和阻燃剂,以及可选的(F0,发泡剂),尽管相对于组分(a)中的异氰酸酯基团与总和之比,其异氰酸酯指数保持在30-180与组分(b)和(f)中存在的异氰酸酯基反应。还描述了生产这种材料espumados的方法及其在复合结构部件中的用途。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号