The present invention is to separate the fine kaolin and plagioclase (calcite feldspar) and quartz, such as mined domestic kaolinite, dry and crushed mined kaolinite, and separated through a sieve, the granulated product of more than 150 mesh By refining and pulverizing, powders of 300 mesh or more and 150 mesh or less are used for glass raw materials and feeds, and powders of 325 mesh or less are manufactured as industrial powders, which can be used for rubber, plastic atstyle and general plastic fillers. The fine-grained product of 150 mesh or less among the products for which the product is manufactured and the ore is pulverized is finely pulverized after magnetic screening and manufactured into fine powder having an average particle size of d 90 = 6.2 μm and d 50 = 2.0 μm. It is characterized in that it is made of a hiding rate improving filler for paint by improving the physical properties of the powder by reducing firing at ℃.
机译:本发明是分离细的高岭土和斜长石(方解石长石)和石英,例如开采的家用高岭石,干燥和粉碎的开采的高岭石,并通过筛子分离,将150目以上的粒状产物通过精制和粉碎成粉末。玻璃原料和进料使用300目或更大且150目或更少的粉末,而325目或更少的粉末被制成工业粉末,可用于橡胶,塑料样式和一般塑料填料。在制造该产品并进行矿石粉碎的产品中,将150目以下的细颗粒产品进行磁筛后进行细粉碎,制成平均粒径为d 90 的细粉。 = 6.2μm,d 50 = 2.0μm。其特征在于,它是通过降低温度下的烧成来改善粉末的物理性能,从而提高涂料的遮盖率的填料。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号