The present invention relates to a rearrangement process of a polyphenylene ether and a phenolic compound by reacting the polyphenylene ether (At this time, a specific phenol compound is used) in the solution. Rearrangement reaction can be carried out in toluene or a toluene / alcohol blend. The reaction can be carried out in the presence or absence of a catalyst.; A polyphenylene ether with a phenol compound by reacting a polyphenylene ether grown thermal loading method in the solution,; Polyphenylene ether is reacted with a phenolic compound of formula (III) (wherein the phenolic rings are disubstituted with methyl groups or ethyl groups in the ortho-position, the group X is separated from the phenolic ring through at least two carbon atoms, the phenolic compound has a 400g / mole or less, and preferably a molecular weight of less than 300g / mol);; As promoters tree (C 8 -C 10 alkyl) methyl ammonium chloride as phase transfer with a mixture of methanol of 1 to 30% by volume in the presence of a catalyst in toluene and methanol, or toluene and the rearrangement in the same;; Using a diphenoquinone, preferably of 3,3 ', 5,5'-tetramethyl-4,4'-diphenoquinone as a catalyst;; The molar concentration of the phenolic compound in a reaction solution using a method of selecting between 0.9 to 1.1 times the molar quantity of monomeric units in the polyphenylene ether,; 90% or more phenolic compounds may be incorporated in the polyphenylene.
机译:本发明涉及通过使溶液中的聚苯醚(此时,使用特定的苯酚化合物)反应而对聚苯醚和酚化合物进行重排的方法。重排反应可以在甲苯或甲苯/醇混合物中进行。该反应可以在催化剂存在或不存在下进行。通过在溶液中使聚苯醚生长的热负载法反应使聚苯醚与酚化合物反应;聚苯醚与式(III)的酚化合物反应(其中酚环在邻位被甲基或乙基二取代,X基团通过至少两个碳原子与酚环分开)化合物具有400g / mol或更低,优选分子量小于300g / mol;作为促进剂树(C 8 -C 10 烷基),在催化剂存在下,氯化铵与1至30体积%甲醇混合物的相转移。甲苯和甲醇,或甲苯及其重排;使用二苯醌,优选3,3′,5,5′-四甲基-4,4′-二苯醌作为催化剂;使用在聚苯醚中单体单元的摩尔量的0.9至1.1倍之间选择的方法,在反应溶液中酚化合物的摩尔浓度;可以将90%或更多的酚类化合物引入聚苯撑中。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号