首页> 外国专利> USE AS AN IMPROVED ANTI-THEFT MARKING ELEMENT OF IRON-NICKEL SOFT MAGNETIC ALLOYS WITH NANOCRISTALLINE STRUCTURE

USE AS AN IMPROVED ANTI-THEFT MARKING ELEMENT OF IRON-NICKEL SOFT MAGNETIC ALLOYS WITH NANOCRISTALLINE STRUCTURE

机译:用作具有纳米晶界结构的铁-镍软磁合金的改进的防盗标记元素

摘要

The present invention discloses a process for enhancing the harmonic output of a marker comprising the steps of providing an amorphous alloy having a composition (Fe1-xNix)aMb(B1-ySiy)c wherein "x" ranges from about 0.2 to about 0.9, "y" ranges from 0 up to about 0.5, "a" is between about 60 and about 90 atomic %, "b" is between about 0.1 to about 10 atomic %, "c" is between about 0.1 to about 30 atomic percent, and M is at least one metal selected from the group consisting of Mo, Cr, Hf, Nb, Ta, Ti, V, W, and Zr, the amorphous alloy having at least two crystallization temperatures, a first crystallization temperature at which a nanocrystalline phase is formed, and a second crystallization temperature at which a second crystalline phase is formed; annealing the amorphous alloy at a temperature between the first and the second crystallization temperatures for a time sufficient to increase at least one harmonic characteristic of the element. Harmonic markers produced thereby are also disclosed.
机译:本发明公开了一种用于增强标记的谐波输出的方法,该方法包括以下步骤:提供具有组成(Fe1-xNix)aMb(B1-ySiy)c的非晶合金,其中“ x”在大约0.2至大约0.9的范围内, y”的范围是从0到大约0.5,“ a”是大约60到大约90原子%,“ b”是大约0.1到大约10原子%,“ c”是大约0.1到大约30原子%,并且M是选自由Mo,Cr,Hf,Nb,Ta,Ti,V,W和Zr组成的组中的至少一种金属,该非晶态合金具有至少两个结晶温度,第一结晶温度为纳米晶相。形成第二结晶温度,在第二结晶温度下形成第二结晶相。在第一和第二结晶温度之间的温度下对非晶态合金进行退火一段足以增加元素的至少一个谐波特性的时间。还公开了由此产生的谐波标记。

著录项

  • 公开/公告号DE69327403T2

    专利类型

  • 公开/公告日2000-08-03

    原文格式PDF

  • 申请/专利权人 ALLIEDSIGNAL INC. MORRISTOWN;

    申请/专利号DE1993627403T

  • 发明设计人 MARTIS RONALD J.;

    申请日1993-10-15

  • 分类号C22C45/02;H01F1/153;G08B13/24;C22C45/04;

  • 国家 DE

  • 入库时间 2022-08-22 01:40:41