A process for hydrocracking a heavy hydrocarbon oil feedstock, a substantial portion of which boils above 524 DEG C. is described which includes the steps of: (a) passing a slurry feed of a mixture of heavy hydrocarbon oil feedstock and from about 0.01-4.0% by weight (based on fresh feedstock) of coke-inhibiting additive particles upwardly through a confined vertical hydrocracking zone, the hydrocracking zone being maintained at a temperature between about 350 DEG and 600 DEG C. a pressure of at least 3.5 MPa and a space velocity of up to 4 volumes of hydrocarbon oil per hour per volume of hydrocracking zone capacity, (b) removing from the top of the hydrocracking zone a mixed effluent containing a gaseous phase comprising hydrogen and vaporous hydrocarbons and a liquid phase comprising heavy hydrocarbons, (c) passing the mixed effluent into a hot separator vessel, (d) withdrawing from the top of the separator a gaseous stream comprising hydrogen and vaporous hydrocarbons, (e) withdrawing from the bottom of the separator a liquid stream comprising heavy hydrocarbons and particles of the coke-inhibiting additive, and (f) fractionating the separated liquid stream to obtain a heavy hydrocarbon stream which boils above 450 DEG C. said heavy hydrocarbon stream containing said additive particles, and a light oil product. According to the novel feature, at least part of the fractionated heavy hydrocarbon stream boiling above 450 DEG C. is recycled to form part of the heavy hydrocarbon oil feedstock at a lower polarity aromatic oil is added to the heavy hydrocarbon oil feedstock such that a high ratio of lower polarity aromatics to asphaltenes is maintained during hydroprocessing. This provides excellent yields without coke formation.
机译:描述了一种将重质烃油原料加氢裂化的方法,其大部分沸点在524℃以上,其包括以下步骤:(a)使重质烃油原料的混合物的淤浆进料通过,并从约0.01-4.0通过密闭的垂直加氢裂化区向上以重量%计(基于新鲜原料)抑制焦炭的添加剂颗粒,该加氢裂化区保持在约350-600℃的温度下,至少3.5MPa的压力和空间每加氢裂化区容量每小时每小时最多可有4体积碳氢油的速度;(b)从加氢裂化区的顶部除去混合废液,该混合废液包含含有氢和气态烃的气相和含有重烃的液相,( c)将混合流出物送入热的分离器容器,(d)从分离器的顶部抽出包含氢气和气态烃的气流,(e)从分离器的底部中提取包含重烃和抑制焦炭添加剂颗粒的液流,和(f)分馏分离的液流以获得沸点在450℃以上的重烃流。添加剂颗粒和轻油产品。根据该新颖特征,沸腾在450℃以上的至少一部分分馏重烃流被再循环以形成重烃油原料的一部分,在低极性的芳族油被添加到重烃油原料中使得在加氢处理过程中,低极性芳烃与沥青质的比例保持不变。这提供了优异的收率而不形成焦炭。

著录项

  • 公开/公告号DE69609355D1

    专利类型

  • 公开/公告日2000-08-17

    原文格式PDF

  • 申请/专利权人 PETRO-CANADA INC. CALGARY;

    申请/专利号DE19966009355T

  • 发明设计人 BENHAM KELLY;PRUDEN B.;ROY MICHEL;

    申请日1996-12-19

  • 分类号C10G47/26;

  • 国家 DE

  • 入库时间 2022-08-22 01:40:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号