PROBLEM TO BE SOLVED: To simultaneously realize weight reduction and high hardness by providing a double layer structure composed of a white iron structure having a highly hard cam surface and a graphite structure having a soft inner wall of a central hole. ;SOLUTION: A chilled cast iron hollow camshaft for an automobile engine is formed as a double layer structure composed of a white iron structure 3 having the highly hard outer periphery of a cam part and a graphite structure 5 having a soft inner wall part of a hollow hole 4 by inclusion casting of a hollow core. The shaft end is formed so as to have a matrix softer than the graphite structure 5 and excellent in cutting performance. Thus, casting takes an annealing method of placing a heating core or a pad in an end part. Thus, the graphite structure 5 can be sufficiently exhibited by using the hollow core as a core. Graphitization of this part is promoted further by arranging the heating core in the end part, and a soft matrix further transformed into ferrite can be obtained.;COPYRIGHT: (C)2000,JPO
机译:解决的问题:通过提供由具有高硬凸轮表面的白铁结构和具有中心孔内壁的石墨结构组成的双层结构,同时实现重量减轻和高硬度。 ;解决方案:用于汽车发动机的冷铸铁空心凸轮轴形成为双层结构,该双层结构由白铁结构3和石墨结构5组成,白铁结构3的凸轮部分的外周边高度坚硬,而石墨结构5的凸轮的内壁部分较软。通过空心铸件的夹杂铸造形成空心孔4。轴端形成为具有比石墨结构5更软并且切削性能优异的基质。因此,铸造采用将加热芯或垫放置在端部中的退火方法。因此,通过使用中空芯作为芯,可以充分显示石墨结构5。通过在端部设置加热芯,可进一步促进该部分的石墨化,并获得进一步转变为铁素体的软质基体。;版权所有:(C)2000,JPO

著录项

  • 公开/公告号JP3185781B2

    专利类型

  • 公开/公告日2001-07-11

    原文格式PDF

  • 申请/专利号JP19990073845

  • 发明设计人 真殿 統;

    申请日1999-03-18

  • 分类号F16H53/02;B22D15/00;F01L1/04;F16C13/00;

  • 国家 JP

  • 入库时间 2022-08-22 01:34:46

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号