首页> 外国专利> The micro encapsulation curing agent, the production manner, the unsaturated polyester resin constituent which includes the same curing agent, that hardening manner and stabilization manner

The micro encapsulation curing agent, the production manner, the unsaturated polyester resin constituent which includes the same curing agent, that hardening manner and stabilization manner

机译:微囊化固化剂,制造方法,包括相同固化剂的不饱和聚酯树脂成分,固化方式和稳定化方式

摘要

PURPOSE: To obtain the subject curing agent, composed of a core substance of an organic peroxide for an unsaturated polyester resin and a film substance, soluble at a curing temperature and having the inside of a polyelectrolyte and the outside of a specific polymer, excellent in storage stability and pot life and providing sharp curing. ;CONSTITUTION: The objective microencapsulated curing agent is obtained by adding an organic peroxide which is a solid at ordinary temperature and has at least 5°C difference between the melting point and the thermal decomposition temperature for forming a core to an aqueous solution of a substance for forming an inner film containing a polyelectrolyte, producing a liquid mixture at a temperature below the thermal decomposition temperature, then cooling the liquid mixture, forming grains composed of the organic peroxide core and the inner film, subsequently adding a monomer composed of at least one of an acrylic acid ester, a methacrylic acid ester and a vinyl aromatic compound for forming an outer resin film and forming a resin film of the polymerized monomer on the inner film. The above-mentioned curing agent is soluble at the curing temperature of the unsaturated polyester resin and contains the core substance which is the organic peroxide for curing the unsaturated polyester resin in the interior.;COPYRIGHT: (C)1993,JPO&Japio
机译:目的:获得一种目标固化剂,该固化剂由用于不饱和聚酯树脂的有机过氧化物的核心物质和膜状物质组成,在固化温度下可溶并且具有聚电解质的内部和特定聚合物的外部,在储存稳定性和适用期,并提供快速固化。 ;组成:微囊固化的目标固化剂是通过将一种常温下为固体的有机过氧化物添加到一种物质的水溶液中而得到的,该过氧化物在常温下为固体,熔点与形成芯的热分解温度之间的差值至少为5℃。用于形成包含聚电解质的内膜,在低于热分解温度的温度下产生液体混合物,然后冷却该液体混合物,形成由有机过氧化物核和内膜组成的晶粒,随后添加由至少一种构成的单体丙烯酸酯,甲基丙烯酸酯和乙烯基芳族化合物的混合物用于形成外部树脂膜并在内部膜上形成聚合单体的树脂膜。上述固化剂在不饱和聚酯树脂的固化温度下是可溶的,并且包含核心物质,该核心物质是用于在内部固化不饱和聚酯树脂的有机过氧化物。; COPYRIGHT:(C)1993,JPO&Japio

著录项

  • 公开/公告号JP3168627B2

    专利类型

  • 公开/公告日2001-05-21

    原文格式PDF

  • 申请/专利权人 日本油脂株式会社;

    申请/专利号JP19910266948

  • 发明设计人 高村 真澄;氏川 典久;松山 一夫;

    申请日1991-09-19

  • 分类号C08F4/32;C08F4/40;C08F299/04;

  • 国家 JP

  • 入库时间 2022-08-22 01:33:58