PROBLEM TO BE SOLVED: To prepare high-strength high-reactivity coke for blast furnaces without detriment to chamber type coke oven side walls. ;SOLUTION: In this method, 0.05-5 mass % of iron is added to coal, and carbonization proceeds with the coke oven wall temperature kept at 1,100°C or lower. Iron ore or iron dust should be the iron source. It is desired that the coke oven combustion chamber bottom temperature be adjusted so that the coke oven wall surface temperature stay below 1,100°C throughout the entire carbonization period from just after coal injection through just before coke extraction.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:在不损害箱式焦炉侧壁的前提下,为高炉准备高强度高反应活性焦炭。 ;解决方案:在该方法中,将0.05-5质量%的铁添加到煤中,并且在将焦炉壁温度保持在1100℃或更低的条件下进行碳化。铁矿石或铁粉应为铁源。期望调节焦炉燃烧室的底部温度,以使从刚注入煤到焦炭提取之前的整个碳化期间,焦炉壁表面温度保持在1100℃以下。版权所有:(C)2001 ,日本特许厅

著录项

  • 公开/公告号JP2001288477A

    专利类型

  • 公开/公告日2001-10-16

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORP;

    申请/专利号JP20000101657

  • 发明设计人 NOMURA SEIJI;

    申请日2000-04-04

  • 分类号C10B57/04;C10B21/10;C10B47/10;

  • 国家 JP

  • 入库时间 2022-08-22 01:33:38

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号