摘要

PROBLEM TO BE SOLVED: To provide a stainless steel having an excellent adhesion property to a fluororesin having excellent weatherability. ;SOLUTION: The stainless steel having the excellent coating film adhesion property to the fluororesin characterized in that a nonmetallic inclusion containing Mg exists at an area ratio of ≥0.01% within a thickness range of a surface layer of at least 100 μm. The method for manufacturing the same consists in adding 0.0005 to 0.05 mass % Mg into molten stainless steel to deposit Mg oxide or Mg sulfide and subjecting the stainless steel to ordinary hot rolling-descaling-cold rolling-annealing-descaling, then grinding by mechanical polishing to prescribed surface roughness to scalp the Mg in the inclusions and applying a fluororesin coating thereon. The high adhesion property is obtained by the adsorption of the Mg into the inclusion of the fluorine in the coating film.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:提供对耐候性优异的氟树脂具有优异的密合性的不锈钢。 ;解决方案:对氟树脂具有优异的涂膜粘附性的不锈钢,其特征在于,在至少100μm的表面层的厚度范围内,含有Mg的非金属夹杂物的面积比为0.01%。其制造方法是在熔融不锈钢中添加0.0005〜0.05质量%的Mg,使其析出Mg氧化物或Mg硫化物,然后将其进行普通的热轧-除鳞-冷轧-退火-除鳞,然后通过机械研磨进行研磨。达到规定的表面粗糙度,以去除夹杂物中的镁,并在其上涂氟树脂涂层。通过将Mg吸附到涂膜中的氟中而获得高附着力。;版权所有:(C)2001,JPO

著录项

  • 公开/公告号JP2001295073A

    专利类型

  • 公开/公告日2001-10-26

    原文格式PDF

  • 申请/专利权人 NIPPON STEEL CORP;

    申请/专利号JP20000103921

  • 发明设计人 TADOKORO YUTAKA;TAKAHASHI AKIHIKO;

    申请日2000-04-05

  • 分类号C23C26/00;B05D7/14;B05D7/24;

  • 国家 JP

  • 入库时间 2022-08-22 01:32:31

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号