PROBLEM TO BE SOLVED: To provide a preventive conservation method and device that has a simple configuration, and reduces tensile residual stress and sensitization by utilizing thermal shock strain. ;SOLUTION: For the surface region of a welding part in a tensile stress state, the surface region being heated-up by a high-frequency heating coil 1 is quickly cooled by jetting a coolant from a nozzle 11, thus generating transitional temperature difference between the surface region and a part directly under a surface layer, applying tensile thermal shock stress to the surface layer for generating tensile strain, and at the same time for partially allowing the surface layer to yield. Then, cooling is stopped for heat-up for allowing the thermal shock stress to disappear. The surface of the welding part is improved to a state where deformation is elastically returned for relieving tensile stress or a compression residual stress state from a partial yield state. Heating and cooling speed is adjusted, thus reducing the sensitization of welding thermal influence part.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:提供一种预防性的保存方法和装置,其结构简单,并通过利用热冲击应变来减小拉伸残余应力和敏化。 ;解决方案:对于处于拉伸应力状态的焊接部件的表面区域,通过从喷嘴11喷出冷却剂,可以快速冷却被高频加热线圈1加热的表面区域,从而在两者之间产生过渡温度差。表面区域和位于表面层正下方的部分,向表面层施加拉伸热冲击应力以产生拉伸应变,同时使表面层部分屈服。然后,停止冷却以进行加热,以使热冲击应力消失。焊接部的表面被改善为弹性变形的状态,以从局部屈服状态缓和拉伸应力或压缩残余应力状态。调节加热和冷却速度,从而降低了焊接热影响部件的敏感性。;版权所有:(C)2001,日本特许厅

著录项

  • 公开/公告号JP2001141629A

    专利类型

  • 公开/公告日2001-05-25

    原文格式PDF

  • 申请/专利权人 HITACHI LTD;

    申请/专利号JP19990325029

  • 发明设计人 YANAGIDA NOBUYOSHI;

    申请日1999-11-16

  • 分类号G01N3/38;

  • 国家 JP

  • 入库时间 2022-08-22 01:29:40

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号