PROBLEM TO BE SOLVED: To obtain a polyester false twist yarn having excellent stretch back properties, proper bulkiness, high shrinkage/high shrinkage stress free from deepened feeling and to provide a method for producing the polyester false twist yarn. ;SOLUTION: This polyester false twist yarn substantially comprises a polypropylene terephthalate yarn and has characteristics of 10-25% shrinkage percentage in boiling water, 400-800 mg/d shrinkage stress and 90-160°C heat stress peak temperature and false twist crimp. This method for producing the polyester false twist yarn comprises setting a yarn temperature at an outlet of a heater at a room temperature to 100°C in subjecting the polypropylene terephthalate undrawn yarn to drawing and false twist processing.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:为了获得具有优异的回弹性,适当的膨松性,高收缩率/高收缩应力而没有加深的手感的聚酯假捻纱,并提供一种生产聚酯假捻纱的方法。 ;解决方案:这种涤纶假捻纱主要包含对苯二甲酸丙二酯纱,并具有沸水收缩率10-25%,400-800 mg / d的收缩应力和90-160&C的热应力峰值温度和假捻卷曲的特性。 。这种生产聚酯假捻纱的方法包括在将未对苯二甲酸丙二醇酯的未拉伸丝进行拉伸和假捻处理的过程中,将加热器出口处的纱线温度在室温下设定为100℃。COPYRIGHT:(C)2001,日本特许厅

著录项

  • 公开/公告号JP2001098434A

    专利类型

  • 公开/公告日2001-04-10

    原文格式PDF

  • 申请/专利权人 TORAY IND INC;

    申请/专利号JP19990276332

  • 申请日1999-09-29

  • 分类号D02G1/02;D02G1/18;D02G3/04;D02J1/22;

  • 国家 JP

  • 入库时间 2022-08-22 01:27:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号