首页> 外国专利> METHOD OF MAKING AN AS-ROLLED MULTI-PURPOSE WEATHERING STEEL PLATE AND PRODUCT THEREFROM

METHOD OF MAKING AN AS-ROLLED MULTI-PURPOSE WEATHERING STEEL PLATE AND PRODUCT THEREFROM

机译:制备成卷的多用途风化钢板的方法及其制品

摘要

A method of making a weathering grade steel plate includes the steps of establishing a minimum yield strength:plate thickness target from one of 50 KSI:up to 4″, 65 KSI:up to 1.5″, and 70 KSI:up to 1.25″. A modified weathering grade alloy composition is cast into a slab employing effective levels of manganese, carbon, niobium, vanadium, nitrogen, and titanium. The cast slab is heated and rough rolled to an intermediate gauge plate. The intermediate gauge plate is controlled rolled and subjected to one of air cooling or accelerated cooling depending on the minimum yield strength and thickness target. With the controlled alloy chemistry, rolling and cooling, the final gauge plate exhibits discontinuous yielding and can be used for applications requiring a 70 KSI minimum yield strength in plate thicknesses up to 1.25″, a 65 KSI minimum yield strength in plate thickness up to 1.50″ and a 50 KSI minimum yield strength for plates as thick as 4″.
机译:一种制造耐候级钢板的方法包括以下步骤:建立最小屈服强度:钢板厚度目标值从50 KSI:最高4″ 65 KSI:最高1.5″和70 KSI:最高1.25&Prime中的一种: ;。使用有效量的锰,碳,铌,钒,氮和钛将改性的耐候级合金组合物浇铸到板坯中。将铸坯加热并粗轧至中间规格板。根据最小屈服强度和目标厚度,对中间规板进行控制轧制,并进行空气冷却或加速冷却中的一种。通过控制合金的化学成分,轧制和冷却,最终规格的钢板表现出不连续的屈服性,可用于要求厚度不超过1.25&Prime的最小屈服强度为70 KSI,厚度不超过1.25&Prime的最小屈服强度为65 KSI的应用。 1.50″厚度为4″的钢板的最小屈服强度为50 KSI。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号