Anodes zinc cup, process for its preparation and use of the anodes zinc cup for a manganese dry battery

机译:阳极锌杯,其制备方法以及将阳极锌杯用于锰干电池

摘要

The present invention provides a negative electrode for dry cells made of a zinc-based alloy containing 0.004-0.800 wt. % of indium and 0.001-0.25 wt. % of titanium or 0.002-0.500 wt. % of zirconium and significantly containing no such harmful matters as mercury, cadmium, and lead. A method of manufacturing the zinc-can negative electrode by which up to 0.800 wt. % of indium can be added to a zinc-based alloy by hot rolling the alloy within a temperature range from 270 DEG C to 370 DEG C. A manganese dry cell in which a separator coated with a paste containing 0.1-8 wt. % of InCl3 is provided on the internal surface of the zinc can. The zinc can is filled with an anode mixture prepared by adding manganese dioxide and a conductive carbon material such as of acetylene black to an electrolyte containing 35-50 wt. % of ZnCl2. A carbon rod is provided at the center of the anode mixture as a current collector.
机译:本发明提供了一种干电池用负极,该负极由包含0.004至0.800重量%的锌基合金制成。铟和0.001-0.25 wt。钛的%或0.002-0.500 wt。 %的锆,不含任何有害物质,如汞,镉和铅。一种锌罐负极的制造方法,通过该方法可以达到0.800 wt。通过在270℃至370℃的温度范围内对合金进行热轧,可以将%的铟添加到锌基合金中。一种锰干电池,其中隔膜涂覆有包含0.1-8wt。%的糊料。在锌罐的内表面上提供%的InCl 3。锌罐中装有阳极混合物,该混合物是通过将二氧化锰和乙炔黑之类的导电碳材料添加到含35-50 wt。 ZnCl2的%碳棒设置在阳极混合物的中心作为集电器。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号