A method for precipitating nickel and cobalt from an acid aqueous solution containing at least dissolved nickel, cobalt and manganese, comprising adding solid caustic calcined magnesium oxide or freshly slurried caustic calcined magnesium oxide to the solution in an amount sufficient to precipitate a substantial proportion of the nickel and cobalt in solution and to precipitate a minor proportion of the manganese in solution; maintaining the magnesium oxide in contact with the solution for a period of about 1 hour to about 9 hours to thereby achieve precipitation of a substantial proportion of the nickel and cobalt in solution and precipitation of a minor proportion of the manganese in solution; and separating solids precipitated in the prior step from the aqueous solution.
机译:一种从至少含有溶解的镍,钴和锰的酸性水溶液中沉淀镍和钴的方法,该方法包括向溶液中加入固体苛性碱煅烧的氧化镁或新鲜浆化的苛性碱煅烧的氧化镁,其量应足以沉淀出大部分的溶液中的镍和钴,并在溶液中沉淀出少量锰;保持氧化镁与溶液接触约1小时至约9小时的时间,从而实现溶液中大部分镍和钴的沉淀和溶液中少量锰的沉淀;并从水溶液中分离出先前步骤中沉淀的固体。

著录项

  • 公开/公告号FR2766842B1

    专利类型

  • 公开/公告日2001-02-16

    原文格式PDF

  • 申请/专利权人 CENTAUR NICKEL PTY LIMITED;

    申请/专利号FR19980009845

  • 发明设计人 DAVID THOMAS WHITE;

    申请日1998-07-31

  • 分类号C22B3/06;C22B23/00;

  • 国家 FR

  • 入库时间 2022-08-22 01:08:06

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号