PROBLEM TO BE SOLVED: To provide a method for manufacturing a decorated sheet without generating a positional deviation, strain or dimensional change of a precise design pattern by a dry heat after printing or coating in the case of forming a coated layer on a base sheet suitable for deeply contracting stereoscopic process and a method for manufacturing a stereoscopically processed decorated sheet and a stereoscopic shape decorated molding.;SOLUTION: The method for manufacturing the decorated sheet manufactures the sheet having a first coating film layer formed to contain at least a precise design layer having a pattern dimension change allowance rate of 30% or less or a positional accuracy allowance tolerance of ±0.4 mm or less formed on its surface by using only a base sheet having a thermally spoiling temperature of 35 to 180°C as a sheet material under the condition that a drying temperature of the first coating film layer becomes the heat spoiling temperature or higher of the base sheet. In this method, an upper surface of a carrier sheet having higher mold releasability than the drying temperature at the heat spoiling temperature and a lower surface of the base sheet are adhered, the first coating film layer is formed on the upper surface of the base sheet, and then the carrier sheet is released.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:提供一种在适当的基础片材上形成涂层的情况下,在印刷或涂布后不因干热而产生精确设计图案的位置偏差,应变或尺寸变化的装饰片材的制造方法。用于深度收缩立体工艺的方法以及用于制造立体加工的装饰片和立体形状的装饰模制件的方法。解决方案:用于制造装饰片的方法制造具有形成为至少包含精确设计层的第一涂膜层的板通过仅使用具有35至180℃的热损坏温度的基片形成在其表面上的具有30%或更小的图案尺寸变化率比率或≤0.4mm的位置精度容许误差的薄片在第一涂膜层的干燥温度达到热破坏温度以上的条件下基片的在该方法中,将具有比在热损坏温度下的干燥温度高的脱模性的载体片的上表面与基底片的下表面粘合,在基底片的上表面上形成第一涂膜层。 ;然后松开文档装订页。;版权所有:(C)2001,JPO

著录项

  • 公开/公告号JP3325252B2

    专利类型

  • 公开/公告日2002-09-17

    原文格式PDF

  • 申请/专利权人 日本写真印刷株式会社;

    申请/专利号JP20000028994

  • 发明设计人 森 富士男;

    申请日2000-02-07

  • 分类号B44C3/02;B32B31/00;B32B33/00;B41M3/12;

  • 国家 JP

  • 入库时间 2022-08-22 01:02:44

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号