PROBLEM TO BE SOLVED: To obtain a spindle-like light calcium carbonate slurry having low viscosity for both L-viscosity and H-viscosity regardless of a high solid concentration exceeding 70 wt.%, and to provide a method for producing it.;SOLUTION: This method for producing a spindle-like light calcium carbonate slurry comprises a wet-type dispersion treatment process of the spindle-like light calcium carbonate slurry having a solid concentration of 70 to 78 wt.% in which a pre-mixing of a system consisting of spindle-like light calcium carbonate and water mixed with a dispersant by a mixer makes a slurry having 0.5 to 1.5 μm media diameter and 25 to 250 mPa.s viscosity measured by B-type viscometer, and a milling by disk agitating type medium grinding mill is performed at a circumferential speed of the disk satisfying an inequality: 1.1×104 A1/2B-3/4C-1/2D-1≤V≤5.4×104A1/2B-3/4C-1/2D-1 (where A: a medium diameter [mm], B: a viscosity of pre-mixed slurry measured by B-type viscometer [mPa.s], C: a specific gravity of medium [-], D: a filling rate of medium [%], V: circumferential speed of disk [m/s]).;COPYRIGHT: (C)2002,JPO
机译:解决的问题:获得一种纺锤状的轻质碳酸钙浆料,该浆料的L-粘度和H-粘度均低,而不论高固体浓度是否超过70wt。%,并提供一种制备方法。 :该纺锤状轻质碳酸钙浆料的生产方法包括对固形物浓度为70至78重量%的纺锤状轻质碳酸钙浆料进行湿式分散处理工艺,其中将系统预混合由纺锤状轻质碳酸钙和水通过混合器与分散剂混合制成的浆液,其介质直径为0.5至1.5μm,通过B型粘度计测量的粘度为25至250 mPa.s,并通过盘式搅拌进行研磨型介质研磨机以满足以下条件的圆盘的圆周速度进行:1.1×104 A1 / 2B-3 / 4C-1 / 2D-1≤ V≤ 5.4×104A1 / 2B-3 / 4C-1 / 2D-1(其中A:中等直径[mm],B:通过B型粘度计[mPa.s],C:介质的比重[-],D:介质的填充率[%],V:盘的圆周速度[m / s])。版权所有:(C日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号