PROBLEM TO BE SOLVED: To provide a liquid curing accelerator for rapid curing cement/concrete to be efficiently produced and rapidly worked which suppresses rebound of sprayed cement/concrete and separation of materials even in the existence of water, and which can work well even at a place containing air gap such as a crack, and to provide a method of producing the rapid curing cement/ concrete.;SOLUTION: The liquid curing accelerator comprises Al, S, Na and F where 7 to 12 pts.wt. of Al as Al2O3 16 to 22 pts.wt. of S as SO3, 0.4 to 6 pts.wt. of Na as Na2O and 0.5 to 7 pts.wt. of F are contained, in which solid concentration is 20 to 50%, preferably further comprises an organic acid. The rapid curing cement/concrete comprises the liquid curing accelerator and cement/ concrete. The method of producing the rapid curing cement/concrete comprises the steps of feeding the liquid curing accelerator and cement/concrete separately, and mixing them together at the joining point of feeding pipes.;COPYRIGHT: (C)2002,JPO
机译:要解决的问题:提供一种液体固化促进剂,用于快速固化水泥/混凝土,使其高效生产和快速工作,即使在有水的情况下,也能抑制喷涂的水泥/混凝土的回弹和材料的分离,即使在有水的情况下也能很好地工作解决方案:液态固化促进剂包括Al,S,Na和F,其中7至12 pts.wt.。铝作为Al2O3 16至22 pts.wt. S的SO3含量为0.4至6磅Na 2 O 3和0.5至7 pts.wt包含F 1,其中固体浓度为20至50%,优选还包含有机酸。快速固化的水泥/混凝土包括液体固化促进剂和水泥/混凝土。快速固化水泥/混凝土的生产方法包括以下步骤:分别进料液体固化促进剂和水泥/混凝土,并在进料管的连接点将它们混合在一起。;版权所有:(C)2002,日本特许厅

著录项

  • 公开/公告号JP2002047048A

    专利类型

  • 公开/公告日2002-02-12

    原文格式PDF

  • 申请/专利权人 DENKI KAGAKU KOGYO KK;

    申请/专利号JP20000396612

  • 申请日2000-12-27

  • 分类号C04B28/02;B28C5/02;

  • 国家 JP

  • 入库时间 2022-08-22 00:58:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号