SOLIDIFIED CRYSTAL GRAIN FINED STEEL, SOLIDIFIED CRYSTAL GRAIN FINED AUSTENITIC STAINLESS STEEL AND WELDED JOINT THEREOF

机译:凝固的晶粒细化钢,凝固的晶粒细化奥氏体不锈钢及其焊接接头

摘要

PROBLEM TO BE SOLVED: To provide a method for fining the solidified crystal grains of steel for obtaining a slab and a weld metal excellent in low temperature toughness and hot workability and to provide a stainless steel sheet excellent in surface properties by only prescribing components irrelevant to casting (solidifying) conditions.;SOLUTION: In this production method, the solidified craytal grains of steel having a composition containing 0.002 to 0.05% Al, 0.0005 to 0.01% Mg, 0.005 to 0.5% Ti, 0.001 to 0.1% N, 0.001 to 0.1% C and 0.01 to 2.0% Mn, satisfying C+0.015×Mn≤0.09 and also satisfying Ti×N≥0.00003 are refined, or, in this production method, the solidified crystal grains of austenitic stainless steel having a composition containing ≥10.5% Cr and ≥4.0% Ni, and in which, the relation between the Cr equivalent and the Ni equivalent satisfies 0.73×Cr equivalent-Ni equivalent ≥4.4, and also, the range of Ti×N≥0.0005 is satisfied are refined.;COPYRIGHT: (C)2001,JPO
机译:解决的问题:提供一种精炼钢的凝固晶粒的方法,以获得具有优异的低温韧性和热加工性的板坯和焊缝金属,以及通过仅规定不相关的成分来提供表面性能优异的不锈钢板。解决方案:在该生产方法中,钢的凝固后的晶粒由以下组成:Al组成为0.002至0.05%,Mg为0.0005至0.01%,Ti为0.005至0.5%,N为0.001至0.1%,0.001至0.5%。精制0.1%的C和0.01〜2.0%的Mn,满足C + 0.015×Mn≥0.09,并且还满足Ti×N≥0.00003,或者在该制造方法中,使奥氏体系不锈钢的凝固晶粒具有含有&ge的成分。 ; 10.5%Cr和4.0%Ni,其中Cr当量和Ni当量之间的关系满足0.73×Cr当量-Ni当量≥4.4,并且Ti×N的范围为0.0005。感到满意版权:(C)2001,JPO

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号