There is provided a method for recycling synthetic wood materials, transformed into materials through a relatively simple method without performing elimination of encrusted concrete from a previously used sheathing board for use in a concrete form having synthetic wood materials as raw materials. ;The method consists of a step wherein a sheathing board 1 (1a) which had been previously used as a concrete form 50 and formed from synthetic wood materials with a moisture content of less than 15 wt %, wherein between 20 and 75 wt % of cellulose crushed materials, such as wood meal with particle diameters of between 50 and 200 m, and between 25 and 80 wt % of thermoplastic resin molding materials, are mixed, is crushed into numerous coated particles 82, and a step wherein a scraping impact force is applied to each individual coated particle 82, concrete and other encrusted materials encrusted on the previously mentioned coated particles 82 are peeled or separated, and at the same time as the synthetic wood materials constituting the coated particles 82 and the encrusted materials are classified, the particles of the synthetic wood materials are granulated, and the granulated synthetic wood meal materials 83 for which the particles have been granulated are recycled.
机译:本发明提供了一种回收合成木材料的方法,该合成木材料通过相对简单的方法转变成材料,而无需从先前使用的以人造木为原料的混凝土模板中使用的覆板中去除结壳的混凝土。 ;该方法包括一个步骤,其中先前用作混凝土模板 50的护套板 1 1 a 由水分含量低于15 wt%的合成木材料制成,其中20至75 wt%的纤维素压碎材料,例如粒径在50至200 m之间且25在25之间的木粉将80重量%的热塑性树脂成型材料混合,压碎成许多被覆颗粒 82 ,并对每个被覆颗粒 82 ,将包裹在前述涂层颗粒 82 上的混凝土和其他外壳材料剥离或分离,并同时与构成涂层颗粒 82 的合成木材材料和将结皮材料分类,将合成木材料的颗粒造粒,然后将造粒的合成木粉原料 83 已颗粒化的颗粒被回收。

著录项

获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号