首页> 外国专利> A method for Coating of a Hydrophobic Polymer Fibers with Poly (Vinyl alcohol) and coated Fibers composed of a Hydrophobic Polymer, they understand the method.

A method for Coating of a Hydrophobic Polymer Fibers with Poly (Vinyl alcohol) and coated Fibers composed of a Hydrophobic Polymer, they understand the method.

机译:他们了解了用聚乙烯醇涂覆疏水性聚合物纤维的方法以及由疏水性聚合物组成的涂覆纤维的方法。

摘要

A method of coating of a Hydrophobic Polymer Fibers with Poly (Vinyl alcohol), whose method involves providing polu00edmerohidrofobico Fibres,Prepare a solution of Poly (Vinyl alcohol) in waterAnd try polu00edmerohid rofobico Fibers with the solution of Poly (alcoholvinu00edlico) under conditions sufficient to deposit the Poly (Vinyl alcohol) on the surfaces of the Fibers.In some embodiments, the polymer is fibrasde Hydrophobic polyolefin Fibers. For example, the polyolefin Fibres are Fibres of polypropylene or polyethylene.The COP (Vinyl alcohol) is the one which is generally referred to as Poly (Vinyl alcohol) soluble in hot water.Such material is altamentehidrolizado, has a degree of hydrolysis of around 98%. The Molecular Weight of Poly (Vinyl alcohol) will typically of around 10.000, which corresponds approximately to a degree of polymerization of 200.This Invention also provides a method for coating a depolu00edmero Hydrophobic Fibers with Poly (Vinyl alcohol).The Method involves providing Hydrophobic Polymer Fibers.Dissolve Poly (Vinyl alcohol) or at a temperature of at least ededor ALR 60 * c to obtain a solution of Poly (Vinyl alcohol)And Treating the polymer Fibers hidrofobicocon solution of Poly (Vinyl alcohol) under conditions sufficient to deposit the Poly (Vinyl alcohol) on the surfaces of the Fibers.Hydrophobic Polymer Fibers can be lasfibras polyolefin such as polyethylene or polypropylene Fibers.
机译:一种用聚乙烯醇涂覆疏水性聚合物纤维的方法,该方法包括提供聚乙烯醇,制备聚乙烯醇在水中的溶液,然后尝试使用聚乙烯醇溶液制备聚乙烯罗非鱼纤维。在足以将聚(乙烯醇)沉积在纤维表面上的条件下。在一些实施方案中,该聚合物是纤维状疏水聚烯烃纤维。例如,聚烯烃纤维是聚丙烯或聚乙烯的纤维.COP(乙烯醇)是通常被称为可溶于热水的聚乙烯醇。这种材料是altamentehidrolizado,水解度约为98%。聚乙烯醇的分子量典型地为约10,000,这对应于聚合度为200。本发明还提供了用聚乙烯醇涂覆多聚美罗疏水性纤维的方法。提供疏水性聚合物纤维,在至少ededor ALR 60 * c的温度下溶解聚乙烯醇,以得到聚乙烯醇溶液,并在足以满足以下条件的条件下处理聚乙烯醇hidrofobicocon溶液在纤维表面上沉积聚乙烯醇。疏水聚合物纤维可以是小纤维聚烯烃,例如聚乙烯或聚丙烯纤维。

著录项

  • 公开/公告号AR021732A1

    专利类型

  • 公开/公告日2002-07-31

    原文格式PDF

  • 申请/专利权人 KIMBERLY-CLARK WORLDWIDE INC.;

    申请/专利号AR1999P106479

  • 发明设计人

    申请日1999-12-16

  • 分类号D06M15/333;

  • 国家 AR