首页> 外国专利> Process for the catalytic reaction of a mixture containing O2 and SO2 that involves Passing the mixture at temperatures of 350 to 600 degrees Celsius for a First Catalyst V2O5 material and INERYou and at temperatures of 500 to 750 degrees Celsius for a Second Catalyst containing 3 to 30 of ixido 3 to 30 Iron and Arsenic oxide.

Process for the catalytic reaction of a mixture containing O2 and SO2 that involves Passing the mixture at temperatures of 350 to 600 degrees Celsius for a First Catalyst V2O5 material and INERYou and at temperatures of 500 to 750 degrees Celsius for a Second Catalyst containing 3 to 30 of ixido 3 to 30 Iron and Arsenic oxide.

机译:包含O2和SO2的混合物的催化反应的方法,该方法包括:将第一催化剂V2O5材料和INERYou的混合物在350至600摄氏度的温度下通过,将包含3至30的第二催化剂在500至750摄氏度的温度下通过ixido的百分比为3至30%的铁和氧化砷。

摘要

A gas mixture with molecular oxygen and 15 to 60%.SO2 flows through a First Catalyst Layer which contains a catalyst containing Vanadium PENTOXIDE and immediately below through a second layer of CATAlizador containing Catalyst with iron content.The gas mixture is LED into the first Catalyst Layer, which contains granular Catalyst V2O5 and 20% to 80% in PESOD catalytically inactive and Inert material,With Inlet temperature of 350 to 600 degrees C. then leads immediately to the gas mixture in the second layer of Catalyst contains 3 - 30% by weight of arsenic oxide.Gas is a product with a Content of SO3 SO3 ratio in volume; SO2; 0.1 maximum.
机译:具有15%至60%的分子氧的气体混合物,SO2流经第一催化剂层,该催化剂层包含含有五氧化二钒的催化剂,紧接着下方是第二层CATAlizador的第二层,该层包含铁含量的催化剂。含有颗粒状催化剂V2O5和20%至80%的PESOD催化惰性和惰性材料的层,入口温度为350至600摄氏度。然后立即导致第二层催化剂中的气体混合物中含有3-30%气体是指SO3含量与SO3体积比的产品;二氧化硫最多0.1。