A hardened asbestos-free, porous, calcium silicate filler material (50) for an acetylene storage vessel (10) is made by mixing quicklime with water to form a first mixture. Then ground quartz silica is added to form a second mixture. A fibrous reinforcing material is blended in to form a third mixture. A precipitated silica (or synthetic silica) is added and homogenized to form a fourth mixture. The fourth mixture is transferred into a cylinder (10) to be filled and is cured under saturated steam pressure. Thereafter, the cylinder (10) is dried. A gas storage cylinder (10) so formed has a monolithic dry mass (50) filling a metal shell (20). The mass (50) has a porosity of about 88 to 92 %, a density in the range of 250 g/l to 350 g/l, and a crush strength of 250 to 550 psig.
机译:通过将生石灰与水混合以形成第一混合物来制备用于乙炔存储容器(10)的无石棉的多孔硅酸钙硬化填充材料(50)。然后加入研磨的石英二氧化硅以形成第二混合物。混合纤维增强材料以形成第三混合物。添加沉淀的二氧化硅(或合成二氧化硅)并均质以形成第四混合物。将第四混合物转移到缸体(10)中进行填充,并在饱和蒸汽压力下固化。之后,将圆筒(10)干燥。如此形成的储气筒(10)具有填充金属壳(20)的整体式干燥块(50)。团块(50)的孔隙率约为88-92%,密度为250g / l至350g / l,抗碎强度为250-550psig。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号