首页> 外国专利> METHOD FOR PRODUCING HIGH PURITY POTASSIUM FLUOROTANTALATE CRYSTAL OR HIGH PURITY POTASSIUM FLUORONIOBATE CRYSTAL AND RECRYSTALLIZATION VESSEL FOR USE IN THE METHOD FOR PRODUCTION, AND POTASSIUM FLUOROTANTALATE CRYSTAL OR HIGH PURITY POTASSIUM FLUORONIOBATE CRYSTAL PRODUCED BY THE METHOD FOR PRODUCTION

METHOD FOR PRODUCING HIGH PURITY POTASSIUM FLUOROTANTALATE CRYSTAL OR HIGH PURITY POTASSIUM FLUORONIOBATE CRYSTAL AND RECRYSTALLIZATION VESSEL FOR USE IN THE METHOD FOR PRODUCTION, AND POTASSIUM FLUOROTANTALATE CRYSTAL OR HIGH PURITY POTASSIUM FLUORONIOBATE CRYSTAL PRODUCED BY THE METHOD FOR PRODUCTION

机译:制备方法中使用的高纯度氟钛酸钾晶体或高纯度氟硼酸钾结晶和再结晶容器,以及高纯度的氟钛酸钾晶体或磷酸氢二钾

摘要

A method for producing high purity potassium fluorotantalate crystals or high purity potassium fluoroniobate crystals, characterized in that a recrystallization process comprises the first step of cooling a saturated solution from a dissolution process having a temperature of 60 to 90 ° C to a temperature of 35 to 50 ° C at a cooling rate of T ° C/hr, and the second step of cooling the solution from the first step to a temperature of 10 to 20°C at a cooling rate of [T-18] T°C/hr to [T-1] T°C/hr. The method can be used for providing high purity potassium fluorotantalate crystals or high purity potassium fluoroniobate crystals having a good crystal particle diameter distribution which is suitable for producing tantalum or niobium particles for a high capacity capacitor without the use of a physical method for adjusting the particle size thereof.
机译:一种生产高纯度氟钽酸钾晶体或高纯度氟铌酸钾晶体的方法,其特征在于,重结晶过程包括将饱和溶液从温度为60至90℃的溶解过程冷却至温度为35至90的第一步。 50°C以T°C / hr的冷却速率进行,第二步是将溶液从第一步以[T-18] T°C / hr的冷却速率冷却到10至20°C至[T-1]摄氏度/小时。该方法可用于提供具有良好晶体粒径分布的高纯度氟钽酸钾晶体或高纯度氟铌酸钾晶体,其适合于生产用于高容量电容器的钽或铌颗粒,而无需使用用于调节颗粒的物理方法。其大小。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号