The present invention relates to a loess bricks and a manufacturing method and molding apparatus used in my, exterior materials of buildings, hoengto brick is several times ocher other foreign substances removed from the stirred tank 10 to a predetermined particle size in accordance with the present invention pulverized by using one or more conveyor 12 provided with this connecting means for transfer to the hopper (14); Means for input by an appropriate amount into the hopper 14, the yellow earth particles must uniformly mixed by the stirrer 16. At the same time the molding machine 18 of the bottom and transferred to; By a ball pin 24 and the margin of each molded piece (18a) (22a) (32a) provided a yellow soil particles injected into the molding machine 18 in the compression plate 22 during compression of the high-pressure cylinder (150t), (20) high-pressure the method comprising compression molding into a predetermined volume is to be uniformly maintained a uniform intensity delivered; And a ball and a margin angle of each corner, even if the molding is completed through a step of taking out a transport conveyor (46) the bricks from the molding machine 18 by using only the pure yellow earth since the compression molding extrusion molding at a high pressure is formed in the molding process, because the internal cracks and shrinkage prevention, as well as soon as the same time maintaining a uniform compressive strength be a separate drying process is required by the production pallet will be immediately available the masonry and construction.
机译:本发明涉及一种黄土砖及其制造方法和模制设备,其用于建筑物的外部材料,根据本发明,亨特砖是从搅拌罐10中除去的其他异物的数倍于预定的粒径。通过使用一个或多个输送机12将其粉碎,该输送机设有该连接装置以传送至料斗(14);为了以适当的量输入到料斗14中,必须通过搅拌器16将黄土颗粒均匀地混合。在高压缸(150t)的压缩过程中,通过球形销24和每个模制件(18a)(22a)(32a)的边缘提供了在压缩板22中注入到模制机18中的黄色土壤颗粒,( 20)高压包括压模成预定体积的方法是要均匀地保持均匀的强度输送;并且,即使在通过压缩成型挤出成型而仅通过使用纯黄土而从成型机18取出运输机(46)的砖的成型完成的情况下,也形成球和各角的余量角。在成型过程中形成高压,因为防止内部裂缝和收缩,以及在生产托盘需要单独干燥的同时保持均匀的抗压强度,将立即提供砌体和结构。

著录项

  • 公开/公告号KR100314536B1

    专利类型

  • 公开/公告日2001-11-30

    原文格式PDF

  • 申请/专利权人 NULL NULL;

    申请/专利号KR19990036545

  • 发明设计人 정옥민;

    申请日1999-08-31

  • 分类号B28B3/00;

  • 国家 KR

  • 入库时间 2022-08-22 00:31:50

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号