Economic manufacture and product of High strength whangtoh Block

机译:经济型高强度砖头生产

摘要

PURPOSE: An economical manufacturing method of yellow earth blocks with high strength is provided to shorten production time and prevent transformation of products by vibration pressing and steam curing. Accordingly, the method enables to produce a large quantity of blocks and keep the original form in case the blocks are wet. CONSTITUTION: The manufacturing method comprises the steps of: sieving yellow earth(water content: 20-25%) to get powders less than 5mm in size; mixing 87-100wt.% of yellow earth, 0-10wt.% of cement, 0-3wt.% of blast furnace slag; forming by vibration press under the pressure of 6-12kgf/cm¬2 and vibration for 5-10sec.; dry-curing for 4hrs. and steam-curing at 80deg.C. The resultant blocks have 80-120kgf/cm¬2 of compression strength in 1day-curing.
机译:目的:提供一种经济的高强度黄色土块制造方法,以缩短生产时间并防止产品因振动压制和蒸汽固化而变形。因此,该方法使得能够生产大量的块并且在块是湿的情况下保持原始形状。组成:该制造方法包括以下步骤:过筛黄土(水含量:20-25%)以得到小于5mm的粉末;混合87-100wt。%的黄土,0-10wt。%的水泥,0-3wt。%的高炉矿渣;在6-12kgf / cm 2的压力下通过振动压机成型并振动5-10秒。干固化4小时。并在80℃蒸汽固化。所得的块在1天的固化中具有80-120kgf / cm 2的压缩强度。

著录项

  • 公开/公告号KR20020030840A

    专利类型

  • 公开/公告日2002-04-26

    原文格式PDF

  • 申请/专利权人 KIM JIN MAN;

    申请/专利号KR20000061110

  • 发明设计人 CHO SEONG HYEON;KIM DONG JU;KIM JIN MAN;

    申请日2000-10-17

  • 分类号C04B33/00;

  • 国家 KR

  • 入库时间 2022-08-22 00:31:09

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号