PURPOSE: To provide the low-Si, low-P, high-Mn molten iron by increasing the Mn concn. in the molten iron by smelting reduction of Mn ore and subjecting the molten iron to desiliconization and clephosphorization. ;CONSTITUTION: A mixture composed of quicklime and the powdery Mn ore is added to the molten iron tapped from a blast furnace in such a manner that the basicity attains 1.5 to 4.0 to desiliconize the molten iron. In succession, a carbonaceous material and a flux compounded with one or ≥2 kinds of CaF2, Al2O3, and CaCl2 are added together with the mixture composed of the quicklime and the powdery Mn ore to the molten iron after the desiliconization, by which the dephosphorization and the reduction of the Mn ore are simultaneously progressed. As a result, the Mn concn. of the molten iron is increased by using the Si in the molten iron for reduction of the Mn ore without using costly ferromanganese.;COPYRIGHT: (C)1994,JPO&Japio
机译:目的:通过增加锰含量来提供低硅,低磷,高锰铁水。通过熔融还原锰矿石并对铁水进行脱硅和裂磷处理,使铁水中的铁含量降低。组成:将由生石灰和锰粉矿组成的混合物加入到高炉出铁的铁水中,使碱度达到1.5到4.0,以使铁水脱硅。依次将碳质材料和助熔剂与一种或两种以上的CaF 2 ,Al 2 O 3 和CaCl <在进行脱硅处理后,将Sub> 2 与生石灰和锰粉状粉末的混合物一起添加至铁水中,从而同时进行脱磷和锰矿石的还原。结果,Mn浓度。通过使用铁水中的Si还原锰矿石而不使用昂贵的锰铁来增加铁水的含量。;版权:(C)1994,JPO&Japio

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号