PROBLEM TO BE SOLVED: To provide glass of low dielectric constant and low dielectric dissipation factor capable of obtaining a glass fiber suitable for glass fiber fabric to be used for reinforcing material for printed wiring board for high frequency use.;SOLUTION: This low dielectric constant and low dielectric dissipation factor glass has a composition of 48-80% SiO2, 0-18% Al2O3, 11-35% B2O3, 0-10% MgO, 0-10% CaO, 0-7% Li2O+Na2+K2O, and 3% TiO2, in terms of mass%, and H2O is 800 ppm, dielectric constant is ≤0.5 at 1 MHz, and the dielectric dissipation factor is ≤7×10-4.;COPYRIGHT: (C)2003,JPO
展开▼
机译:解决的问题:提供一种低介电常数和低介电损耗因子的玻璃,该玻璃能够获得适用于玻璃纤维织物的玻璃纤维,该玻璃纤维织物将用作高频印刷线路板的增强材料。低介电损耗因子玻璃的成分为48-80%SiO 2 Sub>,0-18%Al 2 Sub> O 3 Sub>,11-35 %B 2 Sub> O 3 Sub>,0-10%MgO,0-10%CaO,0-7%Li 2 Sub> O + Na 2 Sub> + K 2 Sub> O和<3%TiO 2 Sub>(以质量%计),H 2 Sub> O为<800 ppm,在1 MHz时介电常数为&le; 0.5,并且介电损耗因子为&le; 7×10 -4 Sup> .;版权:(C)2003,JPO
展开▼