PROBLEM TO BE SOLVED: To provide a wire for welding austenitic stainless steel which can obtain a weld zone of high quality in which uniform corrosion caused by crude sulfuric acid and pitting corrosion caused by residual chloride ions are evaded at a high efficiency.;SOLUTION: The wire for welding austenitic stainless steel having excellent sulfuric acid corrosion resistance and pitting corrosion resistance has a composition containing, by mass, 0.001 to 0.05% C, 0.01 to 1.5% Si, 0.01 to 2.0% Mn, 21.5 to 28.9% Cr, 7.9 to 13.5% Ni, 2.5 to 4.5% Mo, 2.5 to 4.5% Cu and 0.08 to 0.15% N, and in which the content of P is limited to ≤0.03% and S to ≤0.01%, and also satisfying PI=Cr+3.3×Mo+16×N≥35, GI=-Cr+3.6×Ni+4.7×Mo+11.5×Cu≥65 and a Cr equivalent/an Ni equivalent ≥ 1.90, and the balance iron with inevitable impurities.;COPYRIGHT: (C)2004,JPO
机译:要解决的问题:提供一种用于焊接奥氏体不锈钢的焊丝,该焊丝可以获得高质量的焊接区域,其中可以有效规避由粗硫酸引起的均匀腐蚀和由残留氯离子引起的点蚀的高效率。解决方案:具有优异的耐硫酸腐蚀性和耐点蚀性的奥氏体系不锈钢焊接用焊丝的组成按质量计包含0.001至0.05%C,0.01至1.5%Si,0.01至2.0%Mn,21.5至28.9%Cr,7.9 Ni:13.5%,Mo 2.5-4.5%,Cu 2.5-4.5%,N 0.08-0.15%,其中P的含量限制在0.03%以内,S的含量限制在0.01%以内,并且还满足PI = Cr + 3.3×Mo + 16×N≥ 35,GI = -Cr + 3.6×Ni + 4.7×Mo + 11.5×Cu≥ 65和Cr当量/ Ni当量。 1.90,其余的铁具有不可避免的杂质。;版权所有:(C)2004,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号