PROBLEM TO BE SOLVED: To produce a wire rod for thermal-sprayed coating at a low cost by continuously casting molten Zn-Al base alloy into a bar-state and successively, rolling.;SOLUTION: The molten alloy composed of 0.6-22.0 mass% Al and the balance substantially Zn is continuously cast with a belt and wheel caster provided with an endless belt running while bringing into contact with a rotated casting wheel having a circumferential groove in this peripheral surface under state of covering the circumferential groove so that temperature of the cast material when this material separates from the casting wheel becomes ≤275°C. In succession to the casting, the temperature of the material to be rolled at the inlet of a rolling mill is made to ≤275°C and this material is rolled at ≤275°C while using lubricator emulsion.;COPYRIGHT: (C)2003,JPO
机译:解决的问题:通过连续地将熔融的Zn-Al基合金铸造成棒状并连续轧制,以低成本生产用于热喷涂涂层的线材;解决方案:熔融合金的质量为0.6-22.0在具有覆盖带的轮式连铸机的同时,该带轮式连铸机连续运转,该带轮式连铸机在覆盖该周向槽的状态下在该周向表面中具有周向槽,该周向槽具有旋转的铸造轮,该带轮和带轮连铸机在具有周向槽的温度的状态下连续地铸造%Al和余量基本为Zn。当该材料与铸造轮分离时,铸造材料变为275℃。在铸造之后,使要在轧机入口处轧制的材料的温度达到275℃,并在使用润滑剂乳液的情况下将该材料在275℃下轧制。版权:(C )2003年,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号