The present invention provides a composition comprising a saturated solution of zinc oxide in an aqueous sodium or potassium hydroxide solution wherein the concentrations of the zinc oxide and the sodium hydroxide in said solution are as set forth in FIG. 1, and the concentrations of the zinc oxide and potassium hydroxide are as set forth in FIG. 2. The present invention also provides a process for preparing a solution of zinc oxide in an aqueous base, said process comprising diluting a more concentrated solution of zinc oxide in aqueous sodium or potassium hydroxide to produce a resulting dilute solution of zinc oxide having a concentration of zinc oxide that is higher than that obtained by dissolving solid zinc oxide in aqueous sodium or potassium hydroxide, wherein the concentration of the aqueous sodium or potassium hydroxide used for dissolving the solid zinc oxide is substantially the same as the concentration of the aqueous sodium or potassium hydroxide in the resulting dilute solution of zinc oxide, and wherein the concentration of the aqueous sodium hydroxide in the resulting dilute solution ranges from 5 wt % NaOH to about 35 wt % NaOH, and the concentration of the aqueous potassium hydroxide in the resulting dilute solution ranges from 10 wt % KOH to about 55 wt % KOH. The present invention also provides a process for producing zinc metal comprising electrolyzing a basic solution of zinc oxide prepared by the aforementioned process.
机译:本发明提供一种组合物,其包含氧化锌在氢氧化钠或氢氧化钾水溶液中的饱和溶液,其中所述溶液中氧化锌和氢氧化钠的浓度如图1所示。 1,以及氧化锌和氢氧化钾的浓度如图1所示。 2。 本发明还提供了制备在水性碱中的氧化锌溶液的方法,所述方法包括将更浓的氧化锌溶液在氢氧化钠或氢氧化钾水溶液中稀释以产生具有以下特征的稀释的氧化锌溶液:氧化锌的浓度高于通过将固体氧化锌溶解在氢氧化钠或氢氧化钾水溶液中获得的浓度,其中用于溶解固体氧化锌的氢氧化钠或氢氧化钾水溶液的浓度与水溶液中的浓度基本相同所得的氧化锌稀溶液中的氢氧化钠或氢氧化钾,并且其中所得的稀溶液中氢氧化钠水溶液的浓度为5 wt%NaOH至约35 wt%NaOH,所得稀溶液的范围为10重量%KOH至约55重量%KOH。本发明还提供一种生产锌金属的方法,该方法包括电解通过上述方法制得的氧化锌的碱性溶液。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号