WATER BASED ADHESION PROMOTOR FOR POLYPROPYLENE AND METHOD FOR COATING TO POLYPROPYLENE MATERIALS USING THE PROMOTOR

机译:聚丙烯的水基粘合促进剂和使用该促进剂涂覆聚丙烯材料的方法

摘要

The water base adhesion promotor for polypropylene comprises: a grafted polypropylene chloride, which includes a polypropylene chloride moiety and a maleic anhydride moiety as bonded thereto, and which has a chlorine content of 15~25 weight % and a maleic anhydride moiety content of 1~5 weight %; an amine-neutralized water-soluble resin; a wettability-improving agent; and water; and is characterized by having: a combination ratio of 25~90 weight % as of the grafted polypropylene chloride to the total of the grafted polypropylene chloride and the amine-neutralized water-soluble resin; a combination ratio of 2.5~6.0 weight % as of the wettability-improving agent to the entirety of the promotor; and a solid content of 2~10 weight % of the entirety of the promotor. The method for coating to polypropylene materials comprises: a pretreatment step in which the polypropylene material is beforehand cleaned and then the above water base adhesion promotor is applied, and then dried; and a coating step in which a paint is coated to the material after the pretreatment step.
机译:用于聚丙烯的水基粘合促进剂包括:接枝的聚氯乙烯,其包括结合的聚氯乙烯部分和顺丁烯二酸酐部分,并且其氯含量为15〜25重量%,顺丁烯二酸酐部分含量为1〜。 5重量%;胺中和的水溶性树脂;润湿性改善剂;和水;其特征在于,相对于接枝聚氯乙烯和胺中和的水溶性树脂的总量,接枝聚氯乙烯的组合比例为25〜90重量%。润湿性改善剂的组合比为2.5〜6.0重量%,以促进剂整体为基准。固含量为整个促进剂的2〜10重量%。涂覆到聚丙烯材料上的方法包括:预处理步骤,其中预先清洁聚丙烯材料,然后施加上述水基粘合促进剂,然后干燥;涂覆步骤,其中在预处理步骤之后将涂料涂覆到材料上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号