GERMANIUM-FREE SILICATE WAVEGUIDE COMPOSITIONS FOR ENHANCED L-BAND AND S-BAND EMISSION AND METHOD FOR ITS MANUFACTURE

机译:增强L波段和S波段发射的无锗硅酸盐波导组合物及其制造方法

摘要

A method for manufacturing an optical fiber and the resulting article. The method including the steps of: providing a substrate tube; depositing high purity silica-based cladding layers on the inside of the tube; depositing a germanium-free core comprising a glass including silica, and oxides of Al, La, Er, and Tm; collapsing the substrate tube to form a preform; and drawing the preform to yield an optical fiber. A germanium-free co-doped silicate optical waveguide in accordance with the present invention includes a core material comprising silica, aluminum, lanthanum, erbium and thulium, wherein the concentration of Er is from 15 ppm to 3000 ppm; Al is from 0.5 mol% to 15 mol%; La is less than 2 mol%; and Tm is from 150 ppm to 10000 ppm. In an exemplary specific embodiment the concentration of Al is from 4 mol% to 10 mol%; and the concentration of Tm is from 150 ppm to 3000 ppm. The core may further include F. In an exemplary embodiment, the concentration of F is less than or equal to 6 mol%. The waveguide may be an optical fiber, a shaped fiber or other light-guiding waveguides. An amplifier according to the present invention includes the optical fiber described above.
机译:一种制造光纤的方法和所得制品。该方法包括以下步骤:提供衬底管;在管的内部沉积高纯度的二氧化硅基覆层;沉积包括玻璃的无锗芯,该玻璃包括二氧化硅,以及Al,La,Er和Tm的氧化物;塌陷衬底管以形成预型件;拉伸预制棒以产生光纤。根据本发明的无锗共掺杂硅酸盐光波导包括一种芯材料,该芯材料包括二氧化硅,铝,镧,和th,其中Er的浓度为15ppm至3000ppm。 Al为0.5〜15摩尔%。 La小于2摩尔%; Tm为150ppm〜10000ppm。在一个示例性的具体实施方案中,Al的浓度为4mol%至10mol%;优选为10mol%。 Tm的浓度为150ppm至3000ppm。核可进一步包含F。在一个示例性实施方案中,F的浓度小于或等于6mol%。波导可以是光纤,成形光纤或其他导光波导。根据本发明的放大器包括上述光纤。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号