PROBLEM TO BE SOLVED: To provide a water-cooled copper crucible for the consumable electrode type vacuum arc melting capable of minimizing a cut part by suppressing the generation of defects at the bottom part of an ingot.;SOLUTION: A recessed part 6 having height lower than that of the center part is provided at the peripheral part of the surface of a base board 2 constituting the bottom part of the crucible. The recessed part 6 is an annular groove for example and is designed so that r/R ≥ 0.6 is satisfied when a groove radius is r and an inner radius of the crucible is R. The recessed part is designed so that 0.3 cm ≤α≤ 3.0 cm is satisfied when α is (recessed part volume) / (crucible cross-section area). Since a molten metal generated immediately after the start of melting operation flows into the recessed part 6 and gathers at the peripheral part, the cooling of the molten metal in the crucible is suppressed and the generation of the defects at the bottom part of the ingot is suppressed.;COPYRIGHT: (C)2004,JPO&NCIPI
机译:解决的问题:提供一种用于消耗电极型真空电弧熔化的水冷式铜坩埚,其能够通过抑制铸锭底部的缺陷的产生而使切割部分最小化;解决方案:具有高度的凹入部分6在构成坩埚底部的基板2的表面的周缘部设置有比中央部低的高度。凹部6例如是环状的槽,以r / R&ge = 1的方式设计。当槽半径为r并且坩埚的内径为R时,满足0.6。凹部设计为0.3cm。当α 3.0厘米满足是(凹入部分体积)/(横截面面积)。由于刚开始熔融操作后产生的熔融金属流入凹部6并聚集在周缘部,因此抑制了坩埚中熔融金属的冷却,并且抑制了铸锭底部的缺陷的产生。 ;版权:(C)2004,JPO&NCIPI

著录项

  • 公开/公告号JP2004197222A

    专利类型

  • 公开/公告日2004-07-15

    原文格式PDF

  • 申请/专利权人 SUMITOMO TITANIUM CORP;

    申请/专利号JP20030401610

  • 发明设计人 NANJO JUN;

    申请日2003-12-01

  • 分类号C22B9/20;B22C9/06;B22D7/06;B22D21/06;

  • 国家 JP

  • 入库时间 2022-08-21 23:34:56

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号