PROBLEM TO BE SOLVED: To provide a low shrinkage ultra-high strength concrete composition which is free from occurrence of cracks, and a precast concrete product obtained by using the same with self-filling function.;SOLUTION: An inert fine powder having a Blaine value of 3,000 cm2/g is added to cement of ≥500 kg per 1 m3 of concrete, and the total of the specific surface areas of the cement and the inert fine powder is set to be 250,000 to 500,000 m2.;COPYRIGHT: (C)2004,JPO
机译:解决的问题:提供一种不产生裂纹的低收缩率超高强度混凝土组合物,以及使用该组合物获得的具有自填充功能的预制混凝土产品;解决方案:一种具有Blaine的惰性细粉在每1 m 3 混凝土中添加500 kg水泥时,应添加3,000 cm 2 / g的水泥,水泥和水泥的比表面积之和惰性细粉设定为250,000至500,000 m 2 。;版权:(C)2004,日本特许厅

著录项

  • 公开/公告号JP2004010364A

    专利类型

  • 公开/公告日2004-01-15

    原文格式PDF

  • 申请/专利权人 WAKO CONCRETE KOGYO KK;

    申请/专利号JP20020161694

  • 申请日2002-06-03

  • 分类号C04B28/02;B28B1/00;C04B14/26;C04B20/00;C04B22/06;C04B22/14;C04B24/26;C04B24/32;

  • 国家 JP

  • 入库时间 2022-08-21 23:34:36

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号