METHOD OF PROCESSING WASTE REFRACTORY BRICK FROM COPPER SMELTING FURNACE

机译:用铜熔炼炉加工耐火砖的方法

摘要

PPROBLEM TO BE SOLVED: To provide a method of efficiently disposing, when recovering copper from waste refractory bricks used in a smelting furnace, the waste refractory bricks at a low cost while obviating the necessity of special equipment, such as an autoclave, and preventing the occurrence of biting to a crushing machine such as a crusher. PSOLUTION: The waste refractory bricks are crushed to 50 to 200 mm maximum diameter to separate or expose copper metal impregnated into the inner part, and the copper metal and the resultant crushed matter containing the copper metal are recovered by picking and fed into a converter to undergo recovery of copper. The remaining crushed waste refractory bricks are fed to a slag beneficiation step to undergo further recovery of copper. Moreover, the whole of the crushed waste refractory bricks is fed into the converter to undergo recovery of copper, and then an unmelted portion of the crushed waste refractory bricks in the converter is fed together with converter slag to the slag beneficiation step to undergo further recovery of copper. PCOPYRIGHT: (C)2005,JPO&NCIPI
机译:

要解决的问题:提供一种有效地处置从冶炼炉中使用的废耐火砖中回收铜的方法,以低成本处理废耐火砖,而无需使用高压釜等专用设备,并防止咬到诸如破碎机之类的破碎机。

解决方案:将废耐火砖压碎至最大直径为50至200 mm,以分离或暴露浸入内部的铜金属,然后将铜金属和所得的含铜金属压碎物通过拾取进行回收并送入转炉进行铜的回收。将剩下的碎废耐火砖送入矿渣选矿步骤,以进一步回收铜。此外,将全部粉碎的废耐火砖进料到转炉中进行铜的回收,然后将转炉中的未粉碎的废耐火砖的未熔融部分与转炉炉渣一起进料到炉渣的选矿步骤中进行进一步的回收。铜。

版权:(C)2005,JPO&NCIPI