PROBLEM TO BE SOLVED: To provide a nonheat-treated steel which has suitable toughness within a use temperature range, and is easily fractured and separated not only in the conventional low temperature region including a cryogenic region for liquid nitrogen cooling or the like required by the object to be fractured, but also in an inexpensively reachable low temperature region, and to provide an engaged member fractured and separated at low temperatures.;SOLUTION: The nonheat-treated steel easily fractured and separated at low temperatures has a composition comprising, by mass, 0.15 to 0.35% C, 0.5 to 2.0% Si, 0.5 to 1.5% Mn, 0.03 to 0.15% P, 0.01 to 0.15% S, 0.01 to 0.5% Cu, 0.01 to 0.5% Ni, 0.01 to 1.0% Cr, 0.001 to 0.01% s-Al, 0.005 to 0.035% N, 0.0001 to 0.01% Ca and 0.001 to 0.01% O, and satisfying 0.6≤Ceq≤0.85 and 0≤TTr≤1.5, and the balance Fe with inevitable impurities.;COPYRIGHT: (C)2004,JPO&NCIPI
机译:解决的问题:提供一种非热处理钢,该非热处理钢在使用温度范围内具有合适的韧性,并且不仅在包括用于液氮冷却的低温区域等的常规低温区域中容易断裂和分离,还需要解决以下问题。断裂的目的,但也是在价格便宜的低温区域,并提供一种在低温下断裂和分离的接合构件。;解决方案:在低温下易于断裂和分离的未经热处理的钢,其成分组成按质量计,0.15至0.35%C,0.5至2.0%Si,0.5至1.5%Mn,0.03至0.15%P,0.01至0.15%S,0.01至0.5%Cu,0.01至0.5%Ni,0.01至1.0%Cr,0.001至0.01%s-Al,0.005至0.035%N,0.0001至0.01%Ca和0.001至0.01%O,并满足0.6leCeqle 0.85和0leT Tr ≤ 1.5,和剩余铁中不可避免的杂质。;版权所有:(C)2004,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号