(1) under oxygen non- existing the process which emits the propylene polymer material; The process which manufactures the propylene oxide polymer material which includes all peroxide where (2) it adds to the propylene polymer material which emits the oxygen of the quantity which adjusted, 0.004 volume % to be more 15 volume % discloses the said polymer to the oxygen of a less quantity at temperature of the 40C - the 140C, per kilogram of Pol pyrene polymer material is more than 1mmol; (3) optionally, the propylene oxide polymer material substantially at least it is temperature of the 80C in non oxidation atmosphere, but the process which is heated at the temperature which is lower than the softening point of the said polymer; (4) in non oxidation atmosphere, processing the propylene oxide polymer material, at least with the graft monomer of 1 where it can be polymerized by freely radical kinds, at least under existing of the additive of 1 kinds, (a) at least the hydroxylamine derivative polymerization inhibiter of 1 kinds, and, (b) at least the thio, nitro of 1 kinds, it is selected from halogen substitution aliphatic series and the aromatic compound, or aliphatic series and the aromatic phosphine derivative the process which adjusts the molecular weight of the side chain of the graft monomer which was polymerized; And (5) remaining non it activates free radical in the graft conversion propylene polymer material which is obtained manufacture the graft copolymer which possesses the low molecular weight side chain and with the process which removes unreacted vinyl monomer from the said material.
机译:(1)在不存在氧气的条件下放出丙烯聚合物材料的过程; (2)将上述调整后的氧气量调整为0.004体积%至15体积%以上的氧的丙烯聚合物材料中添加(2),将包含所有过氧化物的环氧丙烷聚合物材料的制造方法公开。在40℃至140℃的温度下,每公斤Pol pyr聚合物材料的数量少于1mmol; (3)任选地,环氧丙烷聚合物材料基本上至少是在非氧化气氛中的80℃的温度,但是在低于所述聚合物的软化点的温度下加热该过程。 (4)在非氧化气氛中,至少在1种添加剂存在的情况下,至少用1种可通过自由基聚合的接枝单体处理环氧丙烷聚合物材料,(a)至少(b)至少一种硫胺,硝基的羟胺衍生物聚合抑制剂,(b)选自卤素取代的脂肪族系列和芳香族化合物,或脂肪族系列和芳香族膦衍生物的调节分子的方法。聚合的接枝单体的侧链重量;并且,(5)残存的非活化在具有低分子量侧链的接枝共聚物和通过从所述材料中除去未反应的乙烯基单体的方法得到的接枝转化丙烯聚合物材料中,自由基活化。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号