Fiber web size and production method and the usage where it confounds and the surface it connects

机译:纤维网的尺寸和生产方法以及混杂的用途和连接的表面

摘要

The absorptivity which includes the web size which the Kevlar confounds it is rinteingu fiber structure low, inside the top surface and the bottom surface at least the fiber of one side the surface it is connected by thermal or adhesive connection and the like. Web size, there being an absorptivity, is density low, there is rinteingu resistance, structural it is possible at high temperature just to maintain characteristic. The structure forms the web size of the Kevlar, makes the fiber of web size confound with needle processing or water-flow confounding processing, etc it is possible to make by connecting the fiber with the web size surface with thermal or adhesive connection.
机译:包括凯夫拉尔认为的纤网尺寸的吸收率低是rinteingu纤维结构,至少在其通过热或粘合剂连接而连接的一侧的表面的顶表面和底表面内。卷筒纸的尺寸,具有吸收性,密度低,具有耐印染性,其结构可以在高温下仅保持特性。该结构形成凯夫拉尔纤维网的尺寸,使纤维网尺寸的纤维通过针刺处理或水流混杂处理而混杂,等等,可以通过将纤维与纤维网尺寸表面通过热或粘合连接来制造。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号