PROBLEM TO BE SOLVED: To obtain a steel with low yield point, excellent in toughness and used for an energy absorption device for building at the time of earthquake, by limiting the relationship among respective quantities of C, Ti, and N, reducing the amount of effective C, and limiting a microstructure to a proper range. ;SOLUTION: The steel has a compositon which consists of, by weight, ≤0.1% C, ≤0.4% Si, $1.5% Mn, ≤0.025% P, ≤0.015% S, ≤0.06% Al, 0.005-0.4% Ti, ≤0.006% N, and the balance iron with inevitable impurities and in which the relationship among respective quantities of C, Ti, and N, expressed in weight percentage, satisfies -0.02%≤C-(Ti-3.4N)/4≤0.01%. Further, the steel has a ferritic structure of ≥95% microstructure and has a crystalline grain size of ≥20 μm by circle equivalent diameter, and the ductile/brittle fracture transition temperature (vTrs) at the V Charpy impact test is regulated to ≤0°C.;COPYRIGHT: (C)1999,JPO
机译:要解决的问题:通过限制C,Ti和N各自的含量之间的关系,从而获得一种屈服点低,韧性优异的钢,并将其用作地震时建筑的能量吸收装置,有效C的值,并将微结构限制在适当范围内。 ;解决方案:该钢具有一种成分,按重量计包括0.1%C,0.4%Si,1.5%Mn,0.025%P,0.015%S,0.06%Al,0.005 -0.4%Ti,-0.006%N,以及具有不可避免杂质的余量铁,其中以重量百分比表示的C,Ti和N各自含量之间的关系满足-0.02%&C;(Ti- 3.4N)/4≤0.01%。此外,该钢的铁素体组织为〜95%,当量圆当量直径的结晶粒径为〜20μm,在V夏比冲击试验中的延性/脆性断裂转变温度(vTrs)为2.0。规定为&0; C;版权:(C)1999,JPO

著录项

  • 公开/公告号JP3540927B2

    专利类型

  • 公开/公告日2004-07-07

    原文格式PDF

  • 申请/专利权人 新日本製鐵株式会社;

    申请/专利号JP19980041027

  • 发明设计人 吉江 淳彦;渡部 義之;

    申请日1998-02-09

  • 分类号C22C38/00;C22C38/14;

  • 国家 JP

  • 入库时间 2022-08-21 23:24:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号