A method for mitigating initiation or propagation of a crack in a surface of a metal component in a boiling water reactor. The method includes the step of injecting a solution or suspension of a pH-adjusting compound into the bulk water of the reactor. The compound has the property of changing the pH of high-temperature water inside the crack from a value outside a predetermined pH range (namely, pH 6.0 to 8.0) to a value within the predetermined pH range without causing any significant change of the bulk water pH. The growth rate of the crack when the crack pH is outside the predetermined pH range is greater than the growth rate of the crack when the crack pH is within the predetermined pH range. IMAGE
机译:一种减轻沸腾水反应器中金属部件表面的裂纹萌生或扩展的方法。该方法包括将pH调节化合物的溶液或悬浮液注入反应器的大量水中的步骤。该化合物具有将裂纹内部的高温水的pH从预定pH范围(即,pH 6.0至8.0)之外的值改变为预定pH范围内的值而不会引起大量水的显着变化的性质。 pH值当裂纹pH在预定pH范围之外时,裂纹的生长速率大于当裂纹pH在预定pH范围内时,裂纹的生长速率。 <图像>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号