PROBLEM TO BE SOLVED: To provide a welding material of a martensite system steel containing about 10.5-14% Cr.;SOLUTION: This material comprises 0.1-1.0% Si, 0.1-4.0% Mn, 9.5-14.0% Cr, 4.0-9.0% Ni, 0.3-4.0% MO, 0.05-0.50% Ti, 0-2.0% W, 0-2.0% Cu, 0.03% or less C, N, and P respectively, 0.01% or less S, and 0.04% or less Al. In the formula: Ni balance (%)=30×%C+0.5×%Mn+%Ni+8.2-1.1(1.5×%Si+%Cr+%Mo), the Ni balance is -0.7-2.0, and also in the formula: Cr equivalence (%)=1.5×%Si+%Cr+%Mo, the Cr equivalence is 11-17.;COPYRIGHT: (C)2000,JPO
机译:解决的问题:提供一种含约10.5-14%Cr的马氏体钢的焊接材料;解决方案:该材料包含0.1-1.0%Si,0.1-4.0%Mn,9.5-14.0%Cr,4.0-9.0 Ni,0.3-4.0%MO,0.05-0.50%Ti,0-2.0%W,0-2.0%Cu,0.03%以下C,N和P,0.01%以下S和0.04%以下啊式中:Ni余量(%)= 30倍;%C + 0.5倍;%Mn +%Ni + 8.2-1.1(1.5倍; Si +%Cr +%Mo),Ni余量为-0.7-2.0。式:Cr当量(%)= 1.5倍;%Si +%Cr +%Mo,Cr当量为11-17 .;版权:(C)2000,日本特许厅

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号