A NbC-added Fe—Mn—Si-based shape memory alloy is provided, showing a shape memory property even if a special treatment such as training is not performed. ;A Fe—Mn—Si-based shape memory alloy containing Nb and C is rolled by 10 to 30% in a temperature range of 500 to 800° C. under austenite condition, then, subjected to an aging treatment by heating in a temperature range of 400 to 1000° C. for 1 minute to 2 hours.
机译:提供了一种添加NbC的Fe-Mn-Si基形状记忆合金,即使不进行诸如训练的特殊处理,也显示出形状记忆性能。含Nb和C的Fe-Mn-Si基形状记忆合金在500-800℃的温度范围内轧制10-30%。然后,在奥氏体条件下,通过在400至1000℃的温度范围内加热进行时效处理。 C. 1分钟到2小时。