The present invention makes the best use of a low-cost chemical composition in providing a high strength and high corrosion resistance stainless steel, which has improved delayed fracture resistance and toughness in particular, for building and construction uses, and as, for example, a stainless steel tapping screw. The present invention is, specifically, a stainless steel and a stainless steel screw with high strength and high toughness and excellent in delayed fracture resistance, characterized by: comprising, by mass, 0.01 to 0.25% of C, 0.05 to 1.0% of Si, 0.1 to 2.0% of Mn, 0.1 to 3.0% of Ni, 11.0 to 16.0% of Cr, 0.01 to 0.15% of N, and 0.01 to 3.0% of Mo; containing, optionally, 0.001 to 0.005% of B and/or one or more of 0.05 to 0.5% of Ti, 0.05 to 0.5% of Nb, and 0.05 to 0.5% of W; having less than 10% of ferrite in the center portion of the material; and having a mixed structure of martensite and 3 to 30% of austenite in the surface layer from the outermost surface to the depth of at least 1 &mgr;m, and a method to produce the same.
机译:本发明在提供高强度和高耐腐蚀性的不锈钢中充分利用了低成本的化学成分,该不锈钢尤其具有用于建筑和建筑用途的高的耐延迟断裂性和韧性,例如,不锈钢自攻螺钉。具体而言,本发明是具有高强度和高韧性且耐延迟断裂性优异的不锈钢和不锈钢螺杆,其特征在于,以质量计包含0.01〜0.25%的C,0.05〜1.0%的Si, Mn的0.1〜2.0%,Ni的0.1〜3.0%,Cr的11.0〜16.0%,N的0.01〜0.15%,Mo的0.01〜3.0%。任选地含有0.001至0.005%的B和/或0.05至0.5%的Ti,0.05至0.5%的Nb和0.05至0.5%的W中的一种或多种;材料中心部分的铁素体含量少于10%;从最外表面到至少1μm的深度,在表层具有马氏体和3〜30%的奥氏体的混合组织及其制造方法。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号