首页> 外国专利> Metal/metal oxide doped oxide catalysts having high deNOx selectivity for lean NOx exhaust aftertreatment systems

Metal/metal oxide doped oxide catalysts having high deNOx selectivity for lean NOx exhaust aftertreatment systems

机译:对贫NOx排气后处理系统具有高deNOx选择性的金属/金属氧化物掺杂氧化物催化剂

摘要

A lean NOx catalyst and method of preparing the same is disclosed. The lean NOx catalyst includes a ceramic substrate, an oxide support material, preferably &ggr;-alumina, deposited on the substrate and a metal promoter or dopant introduced into the oxide support material. The metal promoters or dopants are selected from the group consisting of indium, gallium, tin, silver, germanium, gold, nickel, cobalt, copper, iron, manganese, molybdenum, chromium, cerium, vanadium, oxides thereof, and combinations thereof. The &ggr;-alumina preferably has a pore volume of from about 0.5 to about 2.0 cc/g; a surface area of between about 80 to 350 m2/g; an average pore size diameter of between about 3 to 30 nm; and an impurity level of less than or equal to 0.2 weight percent. In a preferred embodiment the &ggr;-alumina is prepared by a sol-gel method, with the metal doping of the &ggr;-alumina preferably accomplished using an incipient wetness impregnation technique.
机译:公开了一种稀NO x催化剂及其制备方法。贫NOx催化剂包括陶瓷基底,沉积在基底上的氧化物载体材料,优选为-氧化铝,以及引入到氧化物载体材料中的金属促进剂或掺杂剂。金属促进剂或掺杂剂选自铟,镓,锡,银,锗,金,镍,钴,铜,铁,锰,钼,铬,铈,钒,其氧化物及其组合。所述-gg氧化铝的孔体积优选为约0.5至约2.0cc / g。表面积在约80至350m 2 / g之间;平均孔径直径在约3至30nm之间;杂质含量小于或等于0.2重量%。在一个优选的实施方案中,通过溶胶-凝胶法制备β-氧化铝,其中对β-氧化铝的金属掺杂优选使用初期湿润浸渍技术来完成。

著录项

  • 公开/公告号US6706660B2

    专利类型

  • 公开/公告日2004-03-16

    原文格式PDF

  • 申请/专利权人 CATERPILLAR INC;

    申请/专利号US20010024430

  • 发明设计人 PAUL W. PARK;

    申请日2001-12-18

  • 分类号B01J230/00;B01J234/00;B01J234/20;B01J235/80;B01J237/00;

  • 国家 US

  • 入库时间 2022-08-21 23:14:25

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号