首页> 外国专利> Piping for transporting oil or gas, method for extending the useful life of a barrier layer of polyamide in a pipeline to transport oil or gas.Method for rejuvenating a barrier layer of Polyamide Used in a pipeline to transport oil or gas, and method for prolonging the life expectancy of a material of polyamide

Piping for transporting oil or gas, method for extending the useful life of a barrier layer of polyamide in a pipeline to transport oil or gas.Method for rejuvenating a barrier layer of Polyamide Used in a pipeline to transport oil or gas, and method for prolonging the life expectancy of a material of polyamide

机译:用于输送石油或天然气的管道,延长用于输送石油或天然气的管道中的聚酰胺阻隔层的使用寿命的方法,用于使用于输送石油或天然气的管道中的聚酰胺阻隔层再生的方法以及延长方法聚酰胺材料的预期寿命

摘要

"Pipe for transporting oil or gas, method for extending the useful life of a barrier layer of polyamide in a pipe to the Pope the transport of oil or gas.Method for rejuvenating a barrier layer of Polyamide Used in a pipeline to transport oil and gas.And the method to prolong the life expectancy of a material of polyamide.The coating of Polyamide Used in transport submarines or land, such as nylon 11.Are manipulated in such a way that increase the rate of recombination in the chain on the process of fission chain competent.This improves and increases the useful life of a polyamide coating effectively reduced their rate of aging.This can be achieved by incorporation of a chain extender or a desiccant in the interior of the polyamide coating.Incorporating the halves or hydrophobic hydrophobic polymers in the interior of the polyamide coating.Or the proportion of a sheath which is less permeable to water at the inner surface of the polyamide coating.The rejuvenation of the polyamide coating can also be achieved by the heat treatment of the Polyamide Coating by heated air, oil or gas heated.Or other heated liquids which are at a temperature above 100 198 C.The rejuvenation can be improved by the inclusion of a chain extender or a desiccant to an oil, gas or liquid is heated which is exposed to the polyamide coating.
机译:“用于输送石油或天然气的管道,用于延长管道中聚酰胺阻隔层使用寿命的方法,用于向教皇输送石油或天然气。用于使聚酰胺阻隔层再生的方法,用于管道中用于输送石油和天然气的管道气体以及延长聚酰胺材料预期寿命的方法。用于运输潜水艇或陆地的聚酰胺涂层,例如尼龙11。应以提高过程中链重组率的方式进行操作可以延长并延长聚酰胺涂层的使用寿命,有效降低其老化率,这可以通过在聚酰胺涂层内部掺入扩链剂或干燥剂来实现。聚酰胺涂层内部的聚合物;或在聚酰胺涂层的内表面渗入水分较少的护套的比例。也可以通过加热空气,油或气或其他温度超过100 <198> C的加热液体对聚酰胺涂层进行热处理来实现。通过添加扩链剂可以改善再生效果或加热暴露在聚酰胺涂层中的油,气或液体干燥剂。

著录项

  • 公开/公告号BR0115681A

    专利类型

  • 公开/公告日2004-06-29

    原文格式PDF

  • 申请/专利权人 DAVID E. KRANBUEHL;

    申请/专利号BR20010115681

  • 发明设计人 DAVID E. KRANBUEHL;

    申请日2001-11-23

  • 分类号B32B1/00;

  • 国家 BR

  • 入库时间 2022-08-21 23:12:15

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号