"Means of grinding of steel or iron lingotado with high carbon content, and its manufacturing process.The present invention relates to balls of steel or iron lingotado with high carbon content obtained by the centrifugal atomisation in a range of particle size preferably between 3 mm and 12 mm.And with an apparent density greater than 4.3 g / cm ^ 3 ^ making it suitable for use as a means of milling plant of ore milling.The speed of rotation of the centrifuge table 12 can be adjusted between 300 rpm, 1500 rpm.The rate of cooling in a minimum mass ball is greater than 10 198 C / second and depends on the drop height (H1) and the depth of the tank (H2).
机译:具有高碳含量的钢或铁的扁钢的研磨方法及其制造方法。本发明涉及通过离心雾化在优选3mm之间的粒径范围内获得的具有高碳含量的钢或铁的扁钢的球。表观密度大于12毫米,表观密度大于4.3克/厘米^ 3 ^,使其适合用作矿石碾磨的研磨设备。离心机台12的旋转速度可在300 rpm之间进行调节, 1500 rpm。最小质量球中的冷却速率大于10 <198> C / s,并取决于下落高度(H1)和储罐深度(H2)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号