首页> 外国专利> BIAXIALLY ORIENTED POLYPROPYLENE FILM HAVING IMPROVED MIGRATION VALUES.

BIAXIALLY ORIENTED POLYPROPYLENE FILM HAVING IMPROVED MIGRATION VALUES.

机译:具有改进的迁移值的双轴取向聚丙烯薄膜。

摘要

Biaxially oriented polypropylene (BOPP) film with at least one base layer contg. polypropylene (PP) is claimed, in which (a) the isotactic block length between two structural defects is more than 40 (statistical average), (b) the n-heptane-insol. component of the PP has an isotacticity (by 13C-NMR spectrometry) of at least 95%, (c) the mol. wt. ratio Mw/Mn is less than 4, (d) the PP contains less than 1% n-heptane-soluble component, and (e) the overall migration of the film (measured as described in DIN EN V 1186-3) is less than 5. Also claimed is a process for the prodn. of this BOPP film, by heating, compressing and melting the polymers for the different layers in extruders, combining the different melts, extruding through a sheet die, cooling and compacting the film on a take-off roll, and orienting the film by stretching in the machine direction by a factor of (3:1)-(9:1) and at right angles by a factor of (4:1)-(12:1).
机译:具有至少一层基础层的双轴取向聚丙烯(BOPP)薄膜。要求保护的聚丙烯(PP),其中(a)两个结构缺陷之间的等规嵌段长度大于40(统计平均值),(b)正庚烷-溶胶。 PP的等分立构规整度(通过<13C-NMR光谱法)至少为95%,(c)摩尔。重量比率Mw / Mn小于4,(d)PP包含小于1%的正庚烷可溶成分,(e)薄膜的整体迁移率(按DIN EN V 1186-3中的方法测量)较小大于5。还要求保护该产品的过程。通过在挤出机中加热,压缩和熔融用于不同层的聚合物,合并不同的熔体,通过片模挤出,在引出辊上冷却和压实薄膜以及通过拉伸拉伸来定向机器方向的系数为(3:1)-(9:1),直角的角度为(4:1)-(12:1)。

著录项

  • 公开/公告号MXPA96002071A

    专利类型

  • 公开/公告日2004-08-19

    原文格式PDF

  • 申请/专利权人 HOECHST AKTIENGESELLSCHAFT;

    申请/专利号MX19960002071

  • 发明设计人 GUNTER SCHL??GL;

    申请日1996-05-30

  • 分类号B29C47/06;B29C55/12;B29K23/00;B29L7/00;B32B27/18;B32B27/32;C08F8/00;C08F10/06;C08J5/18;C08L23/10;

  • 国家 MX

  • 入库时间 2022-08-21 23:09:51

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号