Method for manufacturing composite deoxidizer of molten steel and the composite deoxidizer by using the mothod thereof

机译:钢水复合脱氧剂的制造方法及使用该方法的复合脱氧剂

摘要

PURPOSE: A composite deoxidizer is provided which has high density by adding a reinforcing element to aluminum matrix, and a method is provided which deoxidizes and alloys molten steel and slag using the composite deoxidizer is provided. CONSTITUTION: In a deoxidizer injected into molten metal during manufacturing of steel and iron, the composite deoxidizer is characterized in that the deoxidizer increases relative specific gravity for molten metal by solidifying aluminum in an iron pipe. The method for treating molten steel using a composite deoxidizer comprises the steps of injecting the composite deoxidizer into molten metal, specific gravity of the composite deoxidizer has an initial density of 0.4 or more compared with density of molten steel by adding a metal reinforcing element to aluminum matrix; and melting the composite deoxidizer into molten metal as continuously increasing relative density of the composite deoxidizer to 1.00 to 1.05. The method for deoxidizing slag using a slag deoxidizer is characterized in that the slag deoxidizer is manufactured by adding 20 to 50 wt.% of additive CaO and 10 to 30 wt.% of reinforcing element iron piece to molten metal of 15 wt.% of Mg and 85 wt.% of Al. The method for deoxidizing slag using a slag deoxidizer is characterized in that slag is deoxidized above the slag deoxidizer by injecting the manufactured slag deoxidizer into slag after manufacturing the slag deoxidizer by adding 20 to 50 wt.% of additive CaO and 10 to 30 wt.% of reinforcing element iron piece to molten metal of 15 wt.% of Mg and 85 wt.% of Al.
机译:目的:通过向铝基质中添加增强元素来提供具有高密度的复合脱氧剂,并且提供一种使用该复合脱氧剂对钢水和炉渣进行脱氧和合金化的方法。组成:在钢铁制造过程中注入熔融金属的脱氧剂中,复合脱氧剂的特征在于,该脱氧剂通过固化铁管中的铝来增加熔融金属的相对比重。使用复合脱氧剂处理钢水的方法包括将复合脱氧剂注入到熔融金属中的步骤,与通过向铝中添加金属增强元素的钢水的密度相比,复合脱氧剂的比重具有0.4或更高的初始密度。矩阵;随着将所述复合脱氧剂的相对密度连续增加到1.00至1.05,将所述复合脱氧剂熔融成熔融金属。使用炉渣脱氧剂对炉渣进行脱氧的方法的特征在于,炉渣脱氧剂是通过向熔融金属中添加15重量%的CaO和20至50重量%的添加剂CaO和10至30重量%的增强元素铁片而制造的。镁和85%(重量)的铝。使用炉渣脱氧剂对炉渣进行脱氧的方法的特征在于,通过在制造炉渣脱氧剂之后,通过添加20至50重量%的添加剂CaO和10至30重量%的添加剂将制造的炉渣脱氧剂注入炉渣中,将炉渣在炉渣脱氧剂上方进行脱氧。相对于熔融金属的15重量%的Mg和85重量%的Al的增强元素铁片的百分比。

著录项

  • 公开/公告号KR100411649B1

    专利类型

  • 公开/公告日2003-12-18

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20020055274

  • 发明设计人 남철우;

    申请日2002-09-12

  • 分类号C21C7/06;

  • 国家 KR

  • 入库时间 2022-08-21 22:50:17